| 恒应力下BaTiO3单晶压痕裂纹的滞后扩展和畴变 |
| 赵显武 褚武扬 宿彦京 李金许 高克玮 乔利杰 |
| 北京科技大学材料物理与化学系; 北京 100083 |
|
| Domain Switching and Delayed Propagation of Indentation Crack in BaTiO3 Single Crystal Under Sustained Stress |
| ZHAO Xianwu; CHU Wuyang; SU Yanjing; LI Jinxu; GAO Kewei; QIAO Lijie |
| Department of Materials Physics and Chemistry; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
赵显武; 褚武扬; 宿彦京; 李金许; 高克玮; 乔利杰 . 恒应力下BaTiO3单晶压痕裂纹的滞后扩展和畴变[J]. 金属学报, 2006, 42(1): 13-18 .
,
,
,
,
,
.
Domain Switching and Delayed Propagation of Indentation Crack in BaTiO3 Single Crystal Under Sustained Stress[J]. Acta Metall Sin, 2006, 42(1): 13-18 .
[1]Hao T H,Gong X,Suo Z.J Mech Phys,1996;44:23 [2]Yang W.Mechatronic Reliability.Beijing:Tsinghua University Press,2001:9(杨卫.力电失效学.清华大学出版社,2001:9) [3]Wang Y,Chu W Y,Su Y J,Qiao L J.Mater Sci Eng,2002;B95:263 [4]Wang R M,Chu W Y,Gao K W,Su Y J,Qiao L J.Mater Lett,2004;58:1811 [5]Yang W,Fang F,Tao M.Int J Solids Struct,2001;38:2203 [6]Busche M J,Hsia K J.Scr Mater,2001;44:207 [7]Fang F,Yang W.Mater Lett,2002;57:198 [8]Zhao X W,Su Y J,Gao K W,Qiao L J,Chu W Y,Acta Metall Sin,2005;41:173(赵显武,宿彦京,高克玮,乔利杰,褚武扬.金属学报,2005;41:173) [9]Fang F,Yang W.Mater Lett,2000;46:131 [10]Newman J C,Raju I S.Eng Fract Mech,1981;15:185 [11]Anstis G R,Chantikul P,Lawn B R,Marshall D B.J Am Ceram Soc,1981;64:533 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|