| 单、多轴混合加载下GH4169合金的高温疲劳特性 |
| 尚德广 陈建华 孙国芹 蔡 能 王建国 王连庆 |
| (北京工业大学机电学院; 北京 100022) |
|
引用本文:
尚德广; 陈建华; 孙国芹; 蔡能; 王建国; 王连庆 . 单、多轴混合加载下GH4169合金的高温疲劳特性[J]. 金属学报, 2005, 41(8): 785-790 .
[1] Yoshitada I, Masao S, Masateru O, Kazunari F. Trans ASME J Eng Mater Technol, 1994; 116: 488 [2] Yang X J, Gao Q, Cai L X, Liu Y J. Ada Metall Sin, 2004; 40: 935 (杨显杰,高庆,蔡力勋,刘宇杰.金属学报,2004;40:935) [3] Hales R, Ainsworth R A. Nucl Eng Design, 1995; 153: 257 [4] Shoichi M, Masao S, Masateru O, Takashi O. J Soc Mater Sci, 1997; 46: 1083 [5] Bertini L. Mater High Temp, 1991; 9: 23 [6] Toshiya N, Tomonari I, Yasuhide A. Trans Jpn Soc Mech Eng, 1990; 56: 15 [7] Maile K, Thelen D, Sheng S. J Nucl Mater, 1990; 171: 108 [8] Lamba H S, Sidebottom O M. Trans ASME J Eng Mater Technol, 1978; 100: 96 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|