HVOF喷涂成形纳米晶FeAl厚涂层的结构和热稳定性
嵇 罡; T.Grosdidier (高泰瑞); 郝胜智; 廖汉林; 董 闯
Laboratoire d' Etudes et de Recherches sur les Matériaux; les Procédés et les Surfaces; EA 3316; Université de Technologie de Belfort-Montbéliard; Site de Sevenans; 90010 Belfort Cedex; France
Microstructure and Thermal Stability of HVOF Spray Formed FeAl Thick Nanocoating
JI Gang; T.GROSDIDIER; HAO Shengzhi; LIAO Hanlin; DONG Chuang
Laboratoire d' Etudes et de Recherches sur les Matériaux; les Procédés et les Surfaces; EA 3316; Université de Technologie de Belfort-Montbéliard; Site de Sevenans; 90010 Belfort Cedex; France
引用本文:

嵇罡; T.Grosdidier; 高泰瑞; 郝胜智; 廖汉林; 董闯 . HVOF喷涂成形纳米晶FeAl厚涂层的结构和热稳定性[J]. 金属学报, 2005, 41(6): 561-567 .
, , , , , . Microstructure and Thermal Stability of HVOF Spray Formed FeAl Thick Nanocoating[J]. Acta Metall Sin, 2005, 41(6): 561-567 .

全文: PDF(485 KB)  
摘要: 采用超音速火焰喷涂(HVOF)成形工艺喷涂球磨粉末, 成功制备了纳米晶FeAl厚涂层(5 mm). 分别利用SEM、图像分析、TEM以及Vickers硬度表征了该涂层的微观结构,并与用相同的喷涂参数和原料粉末制备的纳米晶薄涂层(300 $\mu$m)进行了比较, 研究了不同的喷涂条件对涂层的结构及其硬度的影响. 同时, 探讨了厚涂层的热稳定性. 结果表明, 由于涂层中较好地保留了未融粒子中的纳米晶, 从而在600℃仍能保持原有的高硬度.
关键词 : FeAl合金,  纳米晶厚涂层,  喷涂成形     
Abstract:A thick (5 mm) nanostructured Fe-40Al deposit was successfully elaborated by high velocity oxy-fuel (HVOF) spray forming of milled powder. Its microstructure was investigated by scanning electron microscopy (SEM), quantitative metallography, transmission electron microscopy (TEM), as well as micro-hardness measurements. The obtained results were compared to those of a thin (300 $\mu$m) nanostructured coating produced by the same HVOF spray parameters and feedstock powder in order to study the effect of the processing conditions on the microstructure formation and associated hardness. The thermal stability of the deposit was asserted by heat treatments and hardness measurements. Its high hardness, that is due to the retained nanostructured unmelted powder particles, is retained at temperature as high as 600 ℃.
Key words: FeAl    thick nanocoating    spray forming
收稿日期: 2004-09-14     
ZTFLH:  TG174  
[1]Morris D G.Materials Science Foundations 2.Neuchatel, Switzerland,Trans Tech Publications,1998:1
[2]Senkov O N,Srisukhumbowornchai N,Ovecoglu M L, Froes F H.J Mater Res,1998;13:3399
[3]Morris-Munoz M A,Dodge A,Morris D G.Nanostruct Mater,1999;11:873
[4]Liang X B,Deng Z C,Xu Y,Xu B S.Mater Eng,2002; (11):38 (梁秀兵,邓智昌,许一,徐滨士.材料工程,2002;(11):381
[5]Valiev R Z,Korznikov A V,Mulyukov R R.Mater Sci Eng,1993;A168:141
[6]Segal V M.Mater Sci Eng,1995;A197:157
[7]Inoue A.Materials Science Foundations 4-Sendai,Japan, Trans Tech Publications,1998:1
[8]Inoue A.Mater Sci Eng,2001;A304-306:1
[9]Kear B H,Strutt P R.Nanostruct Mater,1995;6:227
[10]Chen H,Zhou X M,Huang M H,Tao S Y,Ding C X.J Inorg Mater,2003;18:914
[11]Lee J S,Ajdelsztajn L,Kim N J,Lavernia E J.In:Berndt C C,Khor K A,Lugscheider E F,eds.,Thermal Spray 2001:New Surf aces for a New Millennium,Oakland,CA,ASM International,2001:511
[12]Tellkamp V L,Lau M L,Fabel A,Lavernia E J.Nanostruct Mater,1997;9:489
[13]He J H,Ice M,Lavernia E J.Metall Mater Trans,2000; 31A:555
[14]He J H,Ice M,Dallek S,Lavernia E J.Metall Mater Trans, 2000;31A:541
[15]Ye X L,Ma S N,Li C Q,Deng Z C.Chin Surf Eng,2004;17(1):31 (叶雄林,马世宁,李长青,邓智昌.中国表面工程,2004;17(1):311
[16]Grosdidier T,Liao H L,Tidu A.In:Berndt C C,ed.,The 1st Int Thermal Spray Conf (ITSC),Montreal,Canada, ASM International,2000:1341
[17]Grosdidier T,Tidu A,Liao H L.Scr Mater,2001;44:387
[18]Grosdidier T,Liao H L,Lenhard S,Tidu A,Revol S.J Phys IV,2001;11:11
[19]Cell M,Jordan E H,Sohn Y H,Goberman D,Shaw L, Xiao T D.Surf Coat Technol,2001;146-147:48
[20]Goberman D,Sohn Y H,Shaw L,Jordan E,Gell M.Acta Mater,2002;50:1141
[21]Li C Q,Ma S N,Deng Z C,Ye X L.Technol Hot Working, 2003;(6):31 (李长青,马世宁,邓智昌,叶雄林.热加工工艺,2003;(6):31)
[22]Lima R S,Kucuk A,Berndt C C.Mater Sci Eng,2001;A313:75
[23]Lima R S,Kucuk A,Berndt C C.Mater Sci Eng,2002;A327:224
[24]Chen H,Ding C X.J Inorg Mater,2002;17:882 (陈煌,丁传贤.无机材料学报,2002;17:882)
[25]Chen H,Zhou X M,Huang M H,Tao S Y,Ding C X.J Inorg Mater,2003;18:911 (陈煌,周霞明,黄民辉,陶顺衍,丁传贤.无机材料学报,2003;18:911)
[26]Holmes R R,Burns D H,McKechnie T N.Thermal Spray Research and Applications,Proc 3rd National Thermal Spray Conference,Long Beach,CA,ASM International,1990:363
[27]Agarwal A,Mckechnie T,Seal S.J Therm Spray Technol,2003;12:350
[28]Takasugi T,Masahaski N,Izumi N.Acta Metall,1987;35:381
[29]Deevi S C,Sikka V K.Intermetallics,1996;4:357
[30]Baker I,Munroe P R.Int Mater Rev,1997;42:181
[31]Stoloff N S.Mater Sci Eng,1998;A258:1
[32]Gaydosh D J,Draper S L,Noebe R D,Nathal M V.Mater Sci Eng,1992;A150:7
[33]Morris D G,Gunther S.Mater Sci Eng,1996;A208:7
[34]Baccino R,Wolski K,Thevenot F,Lecoze J,Moret F.Ann Chim Sci Mater,1997;22:423
[35]Schneibel J H,George E P,Anderson I M.Intermetallics,1997;5:185
[36]Subramanian R,Schneibel J H.Acta Mater,1998;46:4733
[37]Moret F,Baccino R,Martel P,Guetaz L.J Phys IV,1996;6:281
[38]Munoz-Morris M A,Oca C G,Morris D G.Acta Mater,2003;51:5187
[39]Grosdidier T,Suzon E,Wagner F.Intermetallics,2004;12:645
[40]Gialanella S,Amils X,Baro M D,Delcroix P,le Caer G, Lutterotti L,Surinach S.Acta Mater,1998;46:3305
[41]Yang Y M.PhD Thesis.IPSE,France,1996
[42]Deshpande S,Sampath S,Gouma P I,Herman H.In:Moreau C,Marple B eds.,Thermal Spray 2003:Advancing the Science & Applying the Technology,Orlando,Florida,ASM International,2003:1419
[43]Ji G,Elkedim O,Grosdidier T.Surf Coat Technol,2005;190:406
[44]Ji G,Grosdidier T,Morniroli J P.submitted
[45]Simth M F,Dykhuizen R C,Neiser R A.In:Berndt C C,ed.,Thermal Spray 1997:A United Forum for Scientific and Technological Advances,Indianapolis,IN,ASM International,1997:885
[46]Ji G,Morniroli J P,Grosdidier T.Scr Mater,2003;48:1599
[47]Rieu J,Goux C.Mem Sci Rev Metall,1969;66:869
[48]Amils X,Nogues J,Surinach S,Baro M D,Munoz-Morris M A,Morris D G.Intermetallics,2000;8:805
[49]Jordan J L,Deevi S C.Intermetallics,2003;11:507
[1] 孙蔚; 韩福生; 吴杰 . Fe-Al合金中与Al反位置原子弛豫有关的内耗峰[J]. 金属学报, 2007, 43(3): 311-314 .