| 钢中贝氏体相变机制的研究 |
| 方鸿生 杨志刚 杨金波 白秉哲 |
| (清华大学材料科学与工程系;北京 100084) |
|
引用本文:
方鸿生; 杨志刚; 杨金波; 白秉哲 . 钢中贝氏体相变机制的研究[J]. 金属学报, 2005, 41(5): 449-457 .
[1] Devenport E S, Bain E C. Trans Metall Soc AIME, 1930; 90: 117 [2] Hillert M. Scr Mater, 2002; 47: 137; [3] Hsu T Y, Mou Y W. Acta Metall, 1984; 32: 1469 [4] Mou Y W, Hsu T Y. Metall Trans, 1988; 19A: 1695 [5] Hsu T Y. Metall Trans, 1990; 21A: 811 [6] Kang M K, Yang S P, Guan D H. Bainite in Steel. Shanghai: Shanghai Scientific and Technical Publishers, 1990: 57 (康沫狂,扬思品,管敦惠.钢中贝氏体.上海:上海科学技术 出版社, 1990:57) [7] Yu D G, Wang S D. Therory of the Bainite Transformation. Shanghai: Shanghai Jiaotong University Press, 1998: 79 (俞德刚,王世道.贝氏体相变理论.上海:上海交通大学出版 社,1998:79) [8] Smith G V, Mehl R F. Trans AIME, 1942; 150: 211 [9] Aaronson H I, Wells C. JOM, 1956; 8: 1216 [10] Bhadeshia H K D H, Christian J W. Metall Trans, 1990; 21A: 767 [11] Fang H S, Wang J J, Yang Z G. Prog Nat Sci, 1993; 3: 525 (方鸿生,王家军,杨志刚.自然科学进展, 1993;3:525) [12] Fang H S, Wang J J, Yang Z G, Li C M, Bo X Z, Zheng Y K. Bainite Transformation. Beijing: Science Press, 1999: 512 (方鸿生,王家军,杨志刚,李春明,薄祥正,郑燕康.贝氏体 相变.北京:科学技术出版社, 1999:512) [13] Ko T, Cottrell S A. Iron Steel Inst, 1952; 172: 307 [14] Bo X Z, Fang H S, Wang J J. Mater Trans JIM, 1997; 38: 965 [15] Swallow E, Bhadeshia H K D H. Mater Sci Technol, 1996; 12: 121 [16] Fang H S, Wang J J, Zheng Y K. Metall Mater Trans, 1994; 25A: 2001 [17] Srinivasan G R, Wayman C M. Acta Metall, 1968; 16: 621 [18] Srinivasan G R, Wayman C M. Acta Metall, 1968; 16: 609 [19] Hall M G, Rigsbee J M, Aaronson H I. Acta Metall, 1986; 34: 1419 [20] Weatherly G C, Zhang W Z. Metall Mater Tram, 1994; 25A: 1865 [21] Aaronson H I, Hall M G. Metall Mater Trans, 1994; 25A: 1797 [22] Fang H S, Wang J J, Deng Y K, Yang Z G. Acta Metall Sin, 1993; 29A: 445 (方鸿生,王家军,郑燕康,杨志刚.金属学报, 1993;29A: 445) [23] Fang H S, Bo X Z, Wang J J. Mater Trans JIM, 1998; 39: 1264 [24] Yang Z G, Zhang C, Fang H S, Yang J B, Bai B Z, Wang J J. J Mater Sci Technol, 2001; 17: 433 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|