| 应用连续性方法模拟枝晶生长 |
| 李 强 李殿中 钱百年 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| Modelling of the Dendrite Growth by Using Continuous Method |
| LI Qiang; LI Dianzhong; QIAN Bainian |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
李强; 李殿中; 钱百年 . 应用连续性方法模拟枝晶生长[J]. 金属学报, 2004, 40(6): 634-.
,
,
.
Modelling of the Dendrite Growth by Using Continuous Method[J]. Acta Metall Sin, 2004, 40(6): 634-.
[1] Dilthey U, Pavlik K. In: Thomas B G, Beckermann C eds,Welding and Advanced Solidification Processes-Ⅷ PA,Warrendale:1998:589 [2] Nastac L. Acta Mater, 1999; 47: 4253 [3] Zhu M F, Kim J M, Hong C P. ISIJ Inter, 2001; 41: 992 [4] Cho S H, Okane T, Umeda T. Sci Technol Adv Mater,2001; 2: 241 [5] Cinca G R. Physica A, 2002; 314: 284 [6] Nestler B, Wheeler A A, Garcke H. Comput Mater Sci,2003; 26: 111 [7] Damir J, Gretar T. J Comput Phys, 1996; 123: 127 [8] Udaykumar H S, Mao L. Int J Heat Mass Trans, 2002;45: 4793 [9] Eck C, Knabner P, Korotov S. J Comput Phys, 2002; 178:58 [10] Li Q, Guo Q Y, Li D Z, Qian B N, Li D M, Li R, Zhang P W. Chin Phys Lett, 2004; 21: 143 [11] Kurz W, Giovanola B, Thivedi R. Acta Metall, 1986; 34:823 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|