| 镍基块状非晶合金的晶化动力学行为 |
| 秦凤香;张海峰;陈鹏;李宏;胡壮麒 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
| CRYSTALLIZATION KINETICS OF THE Ni-BASED BULK METALLIC GLASS |
| QIN Fengxiang; ZHANG Haifeng; CHEN Peng; LI Hong; HU Zhuangqi |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
秦凤香; 张海峰; 陈鹏; 李宏; 胡壮麒 . 镍基块状非晶合金的晶化动力学行为[J]. 金属学报, 2004, 40(12): 1285-1289 .
,
,
,
,
.
CRYSTALLIZATION KINETICS OF THE Ni-BASED BULK METALLIC GLASS[J]. Acta Metall Sin, 2004, 40(12): 1285-1289 .
[1] Wang X, Yoshii I, Inoue A, Kim Y, Kim I B. Mater TransJIM, 1999; 40: 1130 [2] Wang X, Yoshii I, Inoue A. Mater Trans JIM, 2000; 41:539 [3] Kawashima A, Habazaki H, Hashimoto K. Mater Sci Eng,2001; A304: 753 [4] Katagiri H, Meguro S, Yamasaki M, Habazaki H, Sato T, Kawashima A, Asami K, Hashimoto K. Gorros Sci, 2001; 43: 183 [5] Lee J K, Kim S H, Yi S H, Kim W T, Kim D H. MaterTrans JIM, 2001; 42: 592 [6] Wang L M, Li C F, Inoue A. Mater Trans JIM, 2001; 42:886 [7] Zhang T, Inoue A. Mater Trans JIM, 2002; 43: 708 [8] Zhang W, Inoue A. Scr Mater, 2003; 48: 641 [9] Yim H C, Xu D H, Johnson W. Appl Phys Lett, 2003; 82:1030 [10] Kissinger H E. Anal Chem, 1957; 29: 1702 [11] Santos D S, Santos D R. J Non-Cryst Solids, 2002; 304:56 [12] Liu L, Wu Z F, Zhang J. J Alloys Gompd, 2002; 339: 90 [13] Johnson W A, Mehl R F. Am Inst Miner Pet Eng, 1939;135: 416 [14] Calka A, Radinski A P. J Mater Res, 1985; 3: 59 [15] Aronin A S, Abrosimova G E, Gurov A F, Kir yanov Y V, Molokanov V V. Mater Sci Eng, 2001; A304-306: 375 [16] Lee J K, Kim W T, Kim D H. Mater Lett, 2003; 57: 1514 [17] Inoue A. Intermetallics, 2000; 8: 455 [18] Gerold U, Wiedenmann A, Bellissent R, Macht M P, Wollenberger H. NanoStruct Mater, 1999; 12: 605l |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|