| 恒电场下BaTiO3陶瓷压痕裂纹的滞后扩展 |
| 王瑞敏;宿彦京; 高克玮; 乔利杰; 褚武扬 |
| (北京科技大学材料物理系; 北京100083) |
|
引用本文:
王瑞敏; 宿彦京; 高克玮; 乔利杰; 褚武扬 . 恒电场下BaTiO3陶瓷压痕裂纹的滞后扩展[J]. 金属学报, 2004, 40(11): 1175-1178 .
[1] Suo Z. Curr Opin Solid State Mater Sci, 1998; 3: 486 [2] Hao T H, Gong X, Suo Z. J Mech Phys Solids, 1996; 44:23 [3] Cao H C, Evans A G. J Am Ceram Soc, 1994; 77: 1783 [4] Kim S J, Jiang Q. Smart Mater Struct, 1996; 5: 321 [5] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. ApplPhys Lett, 2003; 82: 1583 [6] Wang R M, Chu W Y, Su Y J, Gao K W, Liu H, Qiao LJ. Mater Lett, accepted [7] Chantikul P, Anstis G R, Lawn B R, Marshall D B. J AmCeram Soc, 1981A; 64: 533 [8] Michalske T A, Freiman S W. J Am Ceram Soc, 1983; 66:284 [9] Wang Y, Chu W Y, Su Y J. Mater Sci Eng, 2002; B95:263 [10] Wang Y, Chu W Y, Su Y J, Gao K W, Liu H, Qiao L J.Acta Metall Sin, 2002; 39: 182(王毅,褚武扬,宿彦京,高克玮,刘辉,乔利杰.金属学报,2002;39:182) [11] Chantikul P, Anstis G R, Laun B R, Marshall D B. J AmCeram Soc, 1981; 64: 539 [12] Yang W. Mechatronic Reliability, Berlin: Springer-Verlag, 2002: 212(杨 卫.力电失效学,北京:清华大学出版社, 2001:151) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|