Pb1-xSrxTiO3固溶化合物及其热膨胀性 |
陈骏 邢献然 邓金侠 |
北京科技大学物理化学系 100083 |
|
引用本文:
陈骏; 邢献然; 邓金侠 . Pb1-xSrxTiO3固溶化合物及其热膨胀性[J]. 金属学报, 2003, 39(7): 771-774 .
[1] Cheng H F, Lin T F, Hu C T. J Am Ceram Soc, 1993; 76:827 [2] Haayman P W, Dam R W, Klasens H A. German Pat,No.929, 1955: 350 [3] Kuwabara M, Suemura S, Kawahara M. Am Ceram Soc Bull, 1985; 64: 1394 [4] Hamada M, Taguchi H, Masumura H. Jpn Pat, 1988;No. 63-280401, 1988 [5] Iwaya S, Masumura H, Taguchi H. J Electron Ceram Jpn,1988; 5: 33 [6] Wang D J, Li L T, Gui Z L. J Chin Ceram Soc, 1996; 24:585(王德君,李龙土,桂枝轮.硅酸盐学报, 1996; 24: 585) [7] von Hippel A. Dielectrics Materials and Applications.New York: Technology Press, 1954 [8] Lench L, Dove D B. Physics of Electric Ceramics. New York: Marcel Dekker Inc., 1971 [9] Kobayashi J, Ueda R. Phys Rev, 1955; 99: 1900 [10] Alefeld B. Z Phys, 1969; 222: 155 [11] Lee C K, Lin I N, Hu C T. J Am Ceram Soc, 1994; 77:1340 [12] Mary T A, Evans J S O, Sleight A W. Science, 1996; 272:90 [13] Evans J S O, Mary T A, Vogt T. Chem Mater, 1996; 8:2809 [14] Shirane G, Hoshino S. J Phys Soc Jpn, 1951; 6: 265 [15] Taylor D. Br Ceram Trans J, 1985; 84: 181 [16] Xing X R, Deng J X, Zhu Z Q, Liu G R. J Alloys Compd,2002; 353: 1 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|