Please wait a minute...
金属学报  2003, Vol. 39 Issue (2): 113-119     
  论文 本期目录 | 过刊浏览 |
氩离子轰击感生Ni2Al3和NiAl3成分变化的TEM/EDS研究
孙丽;陈厚文;王蓉
北京科技大学材料物理系;北京 100083
A TEM/EDS Investigation on Radiation-Induced Composition Changes of Ni2Al3 and NiAl3 Under Bombardment with Ar+ Ions
SUN Li; CHEN Houwen; WANG Rong
Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083
引用本文:

孙丽; 陈厚文; 王蓉 . 氩离子轰击感生Ni2Al3和NiAl3成分变化的TEM/EDS研究[J]. 金属学报, 2003, 39(2): 113-119 .
, , . A TEM/EDS Investigation on Radiation-Induced Composition Changes of Ni2Al3 and NiAl3 Under Bombardment with Ar+ Ions[J]. Acta Metall Sin, 2003, 39(2): 113-119 .

全文: PDF(274 KB)  
摘要: 在能量为3,5和7 keV的氩离子轰击下,对激冷Ni-50%Al(质量分数)合金薄膜进行减薄,用配备有超薄窗口能谱仪的高分辨电镜观察分析了减薄后样品中两种合金相Ni2Al3和NiAl3r结构和成分变化. 结果表明, 在离子轰击下,合金相Ni2Al3和NiAl3的成分均有变化, Ni含量明显高于合金相化学配比. 随着离子能量的降低,轰击后合金相中Ni含量增加. 在3 keV氩离子轰击下两个相的含Ni量均高达87%(原子分数)左右,在离子轰击过程中初始的NiAl3相点阵结构未发生明显变化,而Ni2Al3的初始结构在3和5 keV氩离子轰击减薄后部分转变为体心立方结构.
关键词 : 离子轰击,  Ni2Al3,  NiAl3,  择优溅射    
Key words:
收稿日期: 2002-10-08     
ZTFLH:  TG111.1  
[1] Bartella J, Oechsner H. Surf Sci, 1983; 126: 581
[2] Betz G, Opitz M, Braun P. Nucl Instrum Methods, 1981;182/183: 63
[3] Wirth Th, Atzrodt V, Lange H. Phys Status Solidi, 1984;82A: 459
[4] Hofmann S, Stepanova M G. Appl Surf Sci, 1995; 90: 227
[5] Baretzky B, Moller W, Taglauer E. Nucl Instrum Methods, 1987; B18: 496
[6] Betz G. Surf Sci, 1980; 92: 283
[7] Liau Z L, Mayer J W, Brown W L, Poate J M J. ApplPhys, 1978; 49: 5295
[8] Wang R, Lu Z L, Ko T. J Mater Sci, 2001; 36: 5645
[9] Lu Z L, Wang R, Ko T, Chen H, Mu X H, Zong B N. Chin J Catal, 1997; 18: 110(陆致龙,王蓉,柯俊,陈桦,慕旭宏,宗保宁,催化学报, 1997;18:110)
[10] Andersen H H. Appl Phys, 1979; 18: 131
[11] Sigmund P. Nucl Instrum Methods, 1987; B27: 1
[12] Shapiro M H, Haff P K, Tombrello T A, Harrison Jr D E,Webb R P. Radial Eff, 1985; 89: 234
[13] Wirth Th, Atzrodt V, Lange H. Phys Status Solidi, 1982;72A: K89
[14] Roush M L, Davarya F, Goktepe O F, Andreadis T D.Nucl Instrum Methods, 1982; 209/210: 67
[15] Wang R, Sun L, Chen H W. to be published
[16] Taylor A, Doyle N J. J Appl Crystallogr, 1972; 5: 210
[1] 陈厚文; 王蓉 . 离子减薄后NiAl3合金相中调制结构的高分辨电子显微学研究[J]. 金属学报, 2008, 44(10): 1153-1156 .
[2] 彭德全; 白新德; 陈宝山 . 锆离子轰击对纯锆腐蚀行为的影响[J]. 金属学报, 2005, 41(2): 185-190 .
[3] 邱少红; 王蓉 . Ni2Al3母合金相碱沥滤生成的镍晶粒成行排列的透射电镜观察[J]. 金属学报, 2002, 38(6): 657-660 .