体心立方金属中位错与间隙原子相互作用的回顾——机械波谱术研究 |
L.B.Magalas |
Akademia Gorniczo-hutnicza; Krakow; Poland |
|
引用本文:
L.B.Magalas . 体心立方金属中位错与间隙原子相互作用的回顾——机械波谱术研究[J]. 金属学报, 2003, 39(11): 1145-1152 .
[1] Snoek J L. Physica, 1939; 6: 591 [2] Snoek J L. Physica, 1941; 8: 711 [3] Snoek J L. Physica, 1942; 9: 862 [4] Schoeck G. Ada Metall, 1963; 11: 617 [5] Ke T S. Scr Metall, 1982; 16: 225 [6] Schoeck G. Scr Metall, 1982; 16: 233 [7] Seeger A. Phys Status Solidis, 1979; 55a: 457 [8] Magalas L B, Dufresne J F, Moser P. J Phys Colloq, 1981;42(C5) : 127 [9] Seeger A. J Phys Colloq, 1981; 42(C5) : 201 [10] Seeger A. Scr Metall, 1982; 16: 241 [11] Ritchie I G. Scr Metall, 1982; 16: 249 [12] Seeger A, Weller M, Diehl J, Pan Z L, Zhang J X, Ke TS. Z Metallkd, 1982; 73: 1 [13] Magalas L B, Moser P, Ritchie I G. J Phys Colloq, 1983;44(C9) : 645 [14] Weller M. J Phys Colloq, 1983; 44(C9) : 63 [15] Magalas L B. In: Gorczyca S, Magalas L B, eds., Internal Friction in Solids, Krakow: Wydawnictwo AGH, 1984: 89 [16] Weller M, Tietze M, Diehl J, Seeger A. Mater Sci Monogr,1984; 20: 215 [17] Magalas L B, Moser P. In: Tarcie wewnetrzne i opoznienia magnetyczne w cialach stalych, 1985; 738: 90 (Katowice, Poland: Prace Naukowe Uniwersytetu Slaskiego w Katowicach, 1985) [18] Ogurtani T 6, Seeger A K. J Appl Phys, 1985; 57: 193 [19] Ogurtani T 6, Seeger A K. J Appl Phys, 1987; 62: 852 [20] Schoeck G. Scr Metall, 1988; 22: 389 [21] Sun L H, Wang Y N, Gu M. In: Ke T S, ed., Proc 9th Int Conf on Internal Friction and Ultrasonic Attenuation in Solids, Beijing: International Academic Publishers, 1990:61 [22] Magalas L B. Introduction to Mechanical Spectroscopy. Lausanne, Switzerland : Ecole Polytechnique Federale de Lausanne, 1990: 140 [23] Ngai K L, Wang Y-N, Magalas L B. J Alloys Compd,1994; 211/212: 327 [24] Wang Y, Gu M, Sun L. Phys Rev, 1994; 50B: 3525 [25] Magalas L B. J Phys IV, 1996; 6: 163 [26] Magalas L B, Ngai K L. ASTM STP 1304, 1997: 189 [27] Magalas L B. Inz Mater, 1998; 3: 198 [28] Magalas L B. Defect Diffus Forum, 2001; 194-199: 115 [29] Seeger A. Z Metallkd, 2002; 93: 760 [30] Magalas L B. Solid State Phenom, 2003; 89: 1 [31] Ogurtani T 6, Gungor M R, Oren E E. J Appl Phys, 2002;91: 1860 [32] Ogurtani T O, Gungor M R, Oren E E. Solid State Phenom, 2003; 89: 141 [33] Ke T S. Trans AIME, 1948; 176: 448-474Sachs G, Baldwin M Jr. Trans AIME, 1948; 176: 474-476 [34] Koster W, Bangert L, Hahn R. Arch Eisenhuttenwes,1954; 25: 569 [35] Finkel'shtein B N, Usova L F, Treatment of Steels and Alloys. Collection 38, Moscow: Moscow Steel Institute, Metallurgizdat, 1956 [36] Kamber K, Keefer D, Wert C. Ada Metall, 1961; 9: 403 [37] Schoeck G, Mondino M. J Phys Soc Jpn, 1963; 18(Suppl.1) : 149 [38] Sugeno T, Sakamoto K, Ino H. J Phys Soc Jpn, 1963;18(Suppl. 1) : 154 [39] Barrand P, Leak G M. Acta Metall, 1964; 12: 1147 [40] Rudee M L, Huggins R A. TMS AIME, 1966; 236: 1662 [41] Petarra D P, Beshers D N. Acta Metall, 1967; 15: 791 [42] Ino H, Sugeno T. Acta Metall, 1967; 15: 1197 [43] Bernshtein M L, Tikhomirova E S. In: Finkel'shtein B N, ed., Relaxation Phenomena in Metals and Alloys, New York: Consultants Bureau, 1963: 211 [44] McGrath J, Rawlings R. Acta Metall, 1966; 14: 1 [45] Petarra D P, Beshers D N. J Appl Phys, 1963; 34: 2739 [46] Barrand P, Leak G M. Acta Metall, 1964; 12: 1147 [47] Nakamura M, Sugeno T. Acta Metall, 1973; 21: 539 [48] Buchanan L E, Kennedy R. In: Lenz D, Lucke K, eds., Internal Friction and Ultrasonic Attenuation in Crystalline Solids, Vol.1, Berlin: Springer-Verlag, 1975: 362 [49] Miner R E, Gibala R, Hultgren F A. Acta Metall, 1976;24: 233 [50] View Point Set No.4:the Cold Work Peak. Scr Metall,1982; 16(4) : 221, 225, 233, 241, 249 [51] Hirth J P. Scr Metall, 1982; 16: 221 [52] Ravera P P, Firrao D, Colombo R L. Scr Metall, 1984; 18:1313 [53] Gribniev V N, Gavriliuk V G, Kusznarieva N P, Prokopi-enko V G. Fiz Met Metalloved, 1976; 42: 578 [54] Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids. New York: Academic Press, 1972 [55] Nowick A S, Berry B S. Relaksatsionnye Javleniya v Kristallach. Moskva: Atomizdat, 1975 (Russian translation from English: Anelastic Relaxation in Crystalline Solids) [56] Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids. New York: Academic Press, 1972: 401 [57] Mondino M, Seeger A. Scr Metall, 1977; 11: 817 [58] Golovin S A. Fiz Met Metalloved, 1978; 45: 810 See also English translation: Phys Met Metallogr, 1979;45: 114 [59] Iwasaki Y, Hashiguchi K. Trans Jpn Inst Met, 1982; 23:243 [60] Magalas L B. In: Tarcie wewnetrzne i opoznienia magne-tyczne w cialach stalych, 1984; 615: 60 (Katowice: PraceNaukowe Uniwersytetu Slaaskiego w Katowicach, Poland, 1984) [61] Gavrilyuk V G, Duz V A, Krymchanskiy I I, Terskikh SA. Phys Met Metallogr, 1984; 58: 173 [62] Berger P, Brunet J C, Bouquet G. Scr Metall, 1985; 19:609 [63] Masse M, Brunet J C, Bouquet G. J Phys Colloq, 1985;46(C10) : 247 [64] Gavrilyuk V G, Yagodzinskiy Yu N. Phys Met Metallogr,1986; 62: 180 [65] Gavrilyuk V G, Duz V A, Sitnik B P, Yagodzinskiy Yu N.Phys Met Metallogr, 1986; 62: 201 [66] Magalas L B, Etienne E, David L, Malinowski T. SolidState Phenom, 2003; 89: 321 [67] Ji J W, Zhao Z Q, He L D, Geng D Q. J Phys Colloq,1985; 46(C10) : 257 [68] Sun Z Q, Han M H. In: Ke T S ed., Proc 9th Int Conf onInternal Function and Ultrasonic Attenuation in Solids,Beijing: International Academic Publishers, 1990: 65 [69] Che Y Y, Liu F D, Zeng G Y, Xu Y C, Ji J W, Hua Q Z,Liu J M, Huang Z R. Acta Metall Sin, 1998; 34: 831(车韵怡,刘芬娣,曾桂仪,许余昌,戢景文,华桥柱,刘建民,黄镇如.金属学报,1998;34:831) [70] Che Y Y, Zeng G Y, Xu Y C, Ji J W. Acta Metall Sin(Engl Lett), 1998; 11: 12 [71] Geng D Q, Wu Y Q, Ji J W, Li C Y. In: Ke T S, ed., Proc 9th Int Conf on Internal Friction and Ultrasonic Attenuation in Solids, Beijing: International Academic Publishers, 1990: 103 [72] Surin A I, Blanter M S. Fiz Met Metalloved, 1970; 29: 199 [73] Parisot J,Ferron G. Phys Status Solidis, 1977; 44a: 549 [74] Bielov M V, Fokin A G, Shermergor T D. Fiz Met Metalloved, 1970; 29: 394 [75] Ke T S. Phys Rev, 1948; 74: 9 [76] Ke T S. Phys Rev, 1948; 74: 16 [77] Ke T S. Phys Rev, 1948; 74: 914 [78] Berry B S. J Phys Chem Solids, 1994; 55: 1479 [79] Historical Reviews. J Alloys Compd, 1994; 211/212: 4 [80] Professor T. S. Ke ?Medalist of ICIFUAS-9. In: Ke T S, ed., Proc 9th Int Conf on Internal Friction and Ultrasonic Attenuation in Solids(Appendix), Beijing: International Academic Publishers, 1990: 627 [81] Ke T S, K'ung C P. Sci Sin, 1955; 4: 55First Published in Chinese in Acta Phys Sin, 1954; 10:365(葛庭燧,孔庆平.物理学报, 1954;10:365) [82] Ke T S, Yung P T, Wang Y N. Sci Sin, 1955; 4: 263First Published in Chinese in Acta Phys Sin, 1955; 11: 91(葛庭燧,容保粹,王业宁.物理学报, 1955;11:91) [83] Ke T S, Wang C M. Sci Sin, 1955; 4: 501First Published in Chinese in Acta Phys Sin, 1955; 11:387(葛庭燧,王其闵.物理学报, 1955;11:387) [84] Ke T S, Tsien C T, Karel M. Sci Sin, 1955; 4: 519First Published in Chinese in Acta Phys Sin, 1955; 11:403(葛庭燧,钱知强,卡列尔·密歇克.物理学报,1955;11:403) [85] Ke T S, Ma Y L. Sci Sin, 1956; 5: 19First Published in Chinese in Acta Phys Sin, 1955; 11: 479(葛庭燧,马应良.物理学报, 1955;11:479) [86] Ke T S, Tsien C T. Sci Sin, 1956; 5: 625First Published in Chinese in Acta Phys Sin, 1956; 12:607(葛庭燧,钱知强.物理学报, 1956;12:607) [87] Yung P T, Ke T S. Sci Sin, 1956; 5: 645First Published in Chinese in Acta Phys Sin, 1956; 12:622(容保粹,葛庭燧.物理学报, 1956;12:622) [88] Schoeck G. Phys Rev, 1956; 102: 1458 [89] Magalas L B, Gorczyca S. J Phys Colloq, 1985; 46(C10) :253 [90] Magalas L B, Ritchie I G, Moser P. In: Tarcie wewnetrzne.i opoznienia magnetyczne w cialach stalych, 1985; 738:80 (Katowice, Poland: Prace Naukowe UniwersytetuSlaskiego w Katowicach, 1985) [91] Rubianes J, Magalas L B, Fantozzi G, San Juan J. J PhysColloq, 1987; 48(C8) : 185 [92] Magalas L B, Niblett D H. J Phys Colloq, 1987; 48(C8) :209 [93] West W A. Trans AIME, 1946; 167: 192 [94] Polder D. Philips Res Rep, 1945; 1: 5 [95] Dijkstra L J. Philips Res Rep, 1947; 2: 357 [96] Cottrell A H, Bilby B A. Proc Phys Soc, 1949; A62: 49 [97] Nabarro F R N. Mechanical Effects of Carbon. Report on the Strength of Solids, London: The Physical Society, 1948: 38 (Proc Conf Held at the H. H. Wills Physical Laboratory, University of Bristol, 7-9 July, 1947) [98] Cottrell A H. Effect of Solute Atoms on the Behavior of Dislocation. Report on the Strength of Solids, London: The Physical Society, 1948: 30 (Proc Conf Held at the H. H. Wills Physical Laboratory, University of Bristol, 7-9 July, 1947) [99] Koster W. Arch Eisenhuttenwes, 1928/29; 2: 503 [100] Koster W. Arch Eisenhuttenwes, 1929/30; 3: 637 [101] Swartz J C. Acta Metall, 1962; 10: 406 [102] Ngai K L. In: Magalas L B, ed., Mechanical Spectroscopy,Kluwer Academic Publishers, 2004, in press [103] Magalas L B. J Alloys Compd, 2000; 310: 269 [104] Magalas L B, Malinowski T. Solid State Phenom, 2003;89: 349 [105] Magalas L B, Kwasniewski J. Solid State Phenom, 2003;89: 335 [106] Magalas L B, Malinowski T, Pilat A. In: Non-Destructive Testing, Zeszyty Problemowe. Badania Nieniszczace, SIMP, 2002; 7: 261 (Warsaw: SIMP, 2002) [107] Magalas L B, Malinowski T. In: Non-Destructive Testing, Zeszyty Problemowe. Badania Nieniszczace, SIMP, 2001; 6: 275 (Warsaw: SIMP, 2001) [108] Magalas L B, Fantozzi G, Rubianes J, Malinowski T. JPhys IV, 1996; 6(C8) : 147 [109] Magalas L B, Malinowski T, Rubianes J, Fantozzi G. Inz Mater, 1998; 3: 356 [110] Ogi H, Ledbetter H, Kim S. Metall Mater Trans, 2001;32A: 1671 [111] Numakura H. Solid State Phenom, 2003; 89: 93 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|