| Mg-Al-Zn-Si合金的显微组织细化 |
| 袁广银 刘满平 王渠东 朱燕萍 丁文江 |
| 上海交通大学金属基复合材料国家重点实验室;上海200030 |
|
引用本文:
袁广银; 刘满平; 王渠东; 朱燕萍; 丁文江 . Mg-Al-Zn-Si合金的显微组织细化[J]. 金属学报, 2002, 38(10): 1105-1108 .
[1] Aghion E, Bronfin B. Materials Science Forium, Magnesium Alloys, 2000; 350-351: 19 [2] Brown R E. Light Met Age, 1996; 54: 50 [3] Humble P. Material Forium, 1997; 21: 45 [4] Yuan G Y, Sun Y S, Zhang W M, et al. Trans Non-ferrous Met Soc China, 2000; 10(4): 469 [5] Yuan G Y, Sun Y S, Ding W J. Scr Mater, 2000; 43: 1009 [6] Yuan G Y, Lu Y Z, Ding W J. Ada Metall Sin, 2001; 37: 23 (袁广银,吕宜振,丁文江等,金属学报,2001;37:23) [7] Schmid E E, Von Oldenburg K, Frommeyer. Z Metallkd,1990; 81: 809 [8] Formmeyer G, Beer S, Von Oldenburg K. Z Metallkd,1994; 85: 372 [9] Turnbull D. J Appl Phys, 1950; 21: 1022 [10] Bramffit B L. Metall Trans 1971; 6: 1258 [11] Smithells, Colin James, Brands, et al. Smithells MetalsReference Book, Butterworths Press, London, 1983 [12] Nussbaum G, Sainfort P, Regazzoni G, et al, Scr Met-all,1989; 23: 1079 [13] Armstrong R, Codd I, Douthwaite R M, et al, Phil Mag, 1962; 7: 45" |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|