| 疲劳Cu单晶驻留滑移带的演化及其内应力场 |
| 杨继红 李勇 李守新 马常祥 王刚 柯伟 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳110016 |
|
引用本文:
杨继红; 李勇; 李守新; 马常祥; 王刚; 柯伟 . 疲劳Cu单晶驻留滑移带的演化及其内应力场[J]. 金属学报, 2001, 37(5): 507-511 .
[1] Hunsche A, Neumann P. Acta Metall, 1986; 34: 207 [2] Antonopoulos J G, L. Brown M, Winter A T. Phil Mag,1976; 34A: 549 [3] Essmann U, Gosele U, Mughrabi H. Phil Mag, 1981; 44A:405 [4] Differt K, Essmann U, Mughrabi H. Phil Mag, 1986; 54A:237 [5] Tanaka K, Mura T. J Appl Mech, 1981; 48: 97 [6] Laird C. Mater Sci Eng, 1976; 22: 231 [7] Basinski S J, Basinski Z S, Howie A. Phil Mag, 1969; 19:899 [8] Basinski Z S, Basinski S J. Prong Mater Sci, 1992; 36: 89 [9] Kuhlmann-Wilsdorf D, Laird C. Mater Sci Eng, 1977;27: 137 [10] Wood P J. Phil Mag, 1973; 28: 155 [11] Rasmussen K V, Pedersen O B. Acta Metall, 1980; 28:1467 [12] Mecke K. Phys Stat Sol, 1974; 25A: 93 [13] Winter A T. Phil Mag, 1978; 37A: 457 [14] Tabata T, Fujita H, Hiraoka M, Onishi K. Phil Mag, 1983;47A: 841 [15] Buchinger L, Stanzl S, Laird C. Phil Mag, 1984; 50A: 275 [16] Pedersen O B, Winter T. Phys Stat Sol, 1995; 149A: 281 [17] Yang J H, Li Y, Li S X, Ma C X, Li G Y. Mater Sci Eng,2001; 299A: 51 [18] Hirth J P, Lothe J. Theory of Dislocation. New York:McGraw-Hill, 1968: 60 [19] Hull D, Bacon D J. Introduction to Dislocation. 3rd ed,Oxford: Pergamon Press 1984: 58) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|