| 低应力/应变幅控制的对称拉压疲劳对Ti-49.6Ni合金相变行为的影响 |
| 胡强 金伟 刘晓鹏 曹名洲 李守新 |
| 中国科学院金属研究所钛合金研究室;沈阳110016 |
|
引用本文:
胡强; 金伟; 刘晓鹏; 曹名洲; 李守新 . 低应力/应变幅控制的对称拉压疲劳对Ti-49.6Ni合金相变行为的影响[J]. 金属学报, 2001, 37(3): 263-266 .
[1] Pelosin V, Riviere A. Metall Trans, 1998; 29A: 1175 [2] Ling H C, Kaplow R. Metall Trans, 1980; 11A: 1977 [3] Michal G M, Moine P, Sinclain R. Acta Metall, 1982; 30:125 [4] Miyazaki S, Igo Y, Otsuka K. Acta Metall, 1986; 34: 2045 [5] Stachowiak G B, McCormick P G. Acta Metall, 1988; 36:291 [6] Miyazaki S, Duerig T W eds., Engineering Aspects ofShape Memorg Alloys, Boston: Butterworth-HeinemamLtd., 1990: 394 [7] Miyazaki S, Imal T, Igo Y, Otsuka K. Metall Trans, 1986;17A: 115 [8] Kawaguchi M, Ohashi Y, Tobushi H. Trans Japan SocMechan Eng, 1989; 3A: 628 [9] Tang W J, Sandstrom R. Mater Design, 1993; 14: 2 [10] Jordan L, Masse M, Collier J Y, Bouquet G. J Phys, 1994;4: 157 |
|