| 利用拉伸曲线测定应变诱发马氏体相变能 |
| 张旺峰 陈瑜眉 朱金华 |
| 北京航空材料研究院;北京100095 |
|
引用本文:
张旺峰; 陈瑜眉; 朱金华 . 利用拉伸曲线测定应变诱发马氏体相变能[J]. 金属学报, 2001, 37(10): 1023-1026 .
[1] Cohen M. Trans Metall Soc AIME 1958; 208: 171 [2] Cohen M. Mater Sci Eng, 1983; (2): 34(Cohen M. 材料科学与工程, 1983; (2): 34) [3] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897, 1905,1915 [4] Olson G B, Cohen M. Ann Rev Mater Sci, 1981; 11: 1 [5] Olson G. B, Cohen M. Metall Trans, 1975; 6A: 791 [6] Zhang W F, Chen Y M, Zhu J H. J Xi'an Jiaotong Univ,1999; 33(10): 64(张旺峰,陈瑜眉,朱金华 西安交通大学学报,1999;33(10):64) [7] Marshall P. Austenitic Stainless Steel: Microstructure andMechanical Properties. London: Applied Science Pubul-ishers, 1984: 27 [8] Xiao J M. Metallography Problem of Stainless Steel. Bei-(肖纪美. 不锈钢的金属学问题.北京:冶金工业出版社,1983:64) [9] Tomota Y, Tamura I. Trans Iron Steel Inst Jpn, 1982; 22:665 [10] Zhang W F, Chen Y M, Zhu J H. Chin J Nonferrous Met,1999; 33(10): 163(张旺峰,陈瑜眉,朱金华.中国有色金属学报,2000; 10(10):163 [11] Deng Y R. Theory of Martensite Transformation. Beijing:Science Press, 1993: 7(邓永瑞. 马氏体转变理论.北京:科学出版社,1993:7) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|