| TIG焊接熔池形状参数的视觉检测 |
| 高进强 武传松 |
| 山东工业大学连接技术研究所;济南 250061 |
|
引用本文:
高进强; 武传松 . TIG焊接熔池形状参数的视觉检测[J]. 金属学报, 2000, 36(12): 1284-1288 .
[1] Kumar S, Bhaaduri S C. Metall Trans, 1994; 25B: 435 [2] Wu C S, Zheng W. Ins J Mated 1997; 9: 166 [3] Wu C S, Dorn L. Acta Metall Sin, 1997; 33: 774(武传松, Dorn L.金属学报, 1997; 33: 774) [4] Pan J L. NewB Letter CMES, 2000; 1: 8(潘际銮.中国机械工程学会会讯,2000;1:8) [5] Kovacevic R, Zhang Y M, Li L. Weld J, 1996; 75: 317s [6] Wu C, Gao J, Li J. Int J Joining Mater, 1999; 11: 18 [7] Gao J Q, Li K H, Wu C S. Weld Technol, 1999; 4: 3(高进强,李克海,武传松.焊接技术,1999;4:3) [8] Song Y L. Ph D Thesis, Tianjin University, 1990(宋永伦.天津大学博士学位论文,1990) [9] Li P J. Ph D Thesis, Harbin Institute of Technology, 1997(李朋九.哈尔滨工业大学博士学位论文,1997) |
|