| Al2O3/Al合金复合材料的蠕变与回蠕变行为 |
| 王浩伟 |
| 上海交通大学金属基复合材料国家重点实验室;上海 200030 |
|
引用本文:
王浩伟 . Al2O3/Al合金复合材料的蠕变与回蠕变行为[J]. 金属学报, 2000, 36(11): 1223-1228 .
[1] Goto S, McLean M. Acta Metall Mater, 1991; 39: 153 [2] Dragone T L, Nix W D. Acta Metall Mater 1992; 40:2781 [3] Dlouhy A, Merk N, Eggeler G. Acta Metall Mater 1993;41: 3245 [4] Dlouhy A, Eggeler G, Merk G. Acta Metall Mater, 1995;43: 535 [5] Goto S, McLean M. Acta Metall Mater, 1991; 39: 165 [6] Goto S, McLean M. Scr Metall, 1989; 23: 2073 [7] Dragone T L, Nix W D. Acta Metall Mater, 1990; 38:1941 [8] Dlouhy A, Eggeler G. Scr Metall Mater 1994; 30: 1161 [9] Vedani M, Gariboldi E. Acta Mater, 1996; 44: 3077 [10] Liu P L, Wang Z G, Wang W L, Toda H, Kobayashi T.Acta Metall Sin, 1997; 33: 1227(刘丕林,王中光,王文龙,户田裕之,小木俊郎.金属学报,1997; 33: 1227) [11] Zhou Y M, Chen Y X, Zhang G D, Fei Z M. Acta MaterCompos Sin, 1996; 13(4): 30 (周耀民,陈王喜,张国定,费铸铭复合材料学报,1996: 13(4): 30) [12] Zhu S J, Lu Y X, Wang Z G, Bi J. J Mater, Eng; 1994; 8-9:85 (朱世杰,吕毓雄,王中光,毕敬材料工程, 1994; 8-9: 85) [13] Chen H R,YuanB,Zheng C L.Fiber,Reinf Plast/Compos, 1995; 2:3 (陈浩然,袁彪,郑长良,玻璃钢/复合材料,1995;2:3) [14] Papadakis E P.J Appl Phys, 1964; 35: 1474 [15] Bidlingmaier T, Vogt D, Wanner A, Arzt E. In: AldlingerF, Mughrabi H eds, Proc Werkstoffwoche'96, Sympos 7:Materialwissenschaftliche Grundlagen, Frankfurt: DGM- informationsgesellschafet mbH, 1996: 493 [16] Mills M J, Gibeling J C, Dix W D. In: McQueen H J ed,Proc 7th Int Conf on the Strength of Metals and Alloys,Oxford: Pergamon Press, 1985: 767 [17] Mills M J, Gibeling J C, Dix W D. Acta Metall, 1986; 34:915H |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|