| 合成电子衍射花样的计算机模拟及应用 |
| 鲁世强 罗子健 王仁卉 曾凡昌 |
| 南昌航空工业学院材料系; 南昌 330034 |
|
引用本文:
鲁世强; 罗子健; 王仁卉; 曾凡昌 . 合成电子衍射花样的计算机模拟及应用[J]. 金属学报, 1999, 35(5): 554-560 .
[1] Kestenbach H J. Metallogr, 1977; 10: 189 [2] Assefpour-Dezfuly M, Bonfield W. J Mater Set, 1984; 19:2815 [3] Bowkett M W, Keown S R, Harries D R. Met Set, 1982; 16:499 [4] Rong Y H, Gao M, Wei R P. J Shanghai Jiaotong Univ, 1997;31(4): 27(戎咏华.Gao M, Wei R P. 上海交通大学学报,1997; 31(4):27) [5] Rong Y H, Gao M, Wei R P. Phes Test Chad Anal A: PhysTest, 1997; 33(8): 32(戎咏华,Gao m, wei R P. 理化检验:物理分册,1997; 33(8).32) [6] Alloy Digest inc. Alloy Digest, Orange, June 1990 [7] Graham A H. aams ASM, 1969; 62: 930 [8] Graham A H, YOungblood J L. Metall bens, 1970; 1. 423 [9] Slaney J S, Nebiolo R A. Metall, 1983; 16: 137 [10] Raghavan M, Berkowitz B J, Kane R D. Metall Trans, 1980;11A: 203 [11] Hagan F C, Antes H W. Soperalloys, Warrendale, PA,;TMS-AIME, 1984: 621 [12] Raghavan M, Berkowitz B J. Scs Metall, 1980; 14: 1009 [13] Drapier J M, Viatour P, Coutsouradis D, Habraken L. Cobalt,1970; 49: 171 [14] Smith G D, Yates D H. Met Pad, 1968(3): 100 [15] Singh R P, Doherty R D. Metall fons, 1992; 23A: 307 [16] Singh R P, Doherty R D. Metall aams, 1992; 23A: 321 [17] Slaney J S. US Pat 3767385, 1973 [18] Kline L, Lawler M. Airer Ear, 1989; 61: 2 [19] Kline L, Lawler M. Mater Egg, 1989; 106: 55 [20] Bradley E F. Saperalloys, ASM, Int, 1988: 20 [21] Mao S P, Zhang Y, Chang X, Zhou J. J Mater Egg, 1990; 4:35(马淑波,张匀,常昕,周敬.材料工程,1990; 4: 35) [22] Huang X Y. Transmission Electron Microscopy. Shanghai:Shanghai Science and Technology Press, 1979: 252(黄孝瑛,透射电子显微学.上海:上海科学技术出版社,1979:252) [23] Li S T. X--Ray of Metal and Electron Microscopg Technol-opy. Be1Jing: Metallurgy industry Press, 1980: 363(李树棠.金属X射线与电子显微分析技术,北京:冶金工业出版社, 1980: 363) [24] Hirsch P, Howie A, Nicholso R B, Pashley D W, Whelan MJ. Electron Microscopy of Thin Crystals. New YOrk: RobertE Krieger Publishing Co, 1977: 106 [25] GuangWei H, Di F, Ming Y, Nanseng Y. J Mater Set Technol,1996; 12: 109 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|