| Al-Ti系中间合金的铝热反应 |
| 张柏清 李建国 马洪涛 方鸿生 |
| 清华大学材料科学与工程系;北京 100084 |
|
引用本文:
张柏清; 李建国; 马洪涛; 方鸿生 . Al-Ti系中间合金的铝热反应[J]. 金属学报, 1999, 35(5): 473-476 .
[1] Bondaler B E. US Pat 2857426, 1958 [2] Cibula A. J Inst Met, 1949-50; 76: 321 [3] McCartney D G. Int Mater Red, 1989; 34: 247 [4] Carver R F. Light Met, 1990: 845 [5] Kiusalaas R. Chef Commum, 1986; 1:1 [6] Hu B, Li H. J Mater Process Technol, 1998; 74(1-3): 56 [7] Marcantonio J A, Mondolfo L F. Met aams, 1971; 2: 465 [8] Guzowski M M, Sigworth G K, Sentner D A. Metall TransA, 1987; 18A: 603 [9] Jones G P, Pearson J. Metall Trans, 1976; 7B: 223 [10] Arnberg L, Baeckerud L, Klang H. Met Technol, 1982; 9. 1 [11] Arnberg L, Baeckerud L, Klang H. Met Technol, 1982; 9: 7 [12] Manes C D, McCartney D G, Tatlock G J. Mater Set Tech-nol, 1993; 9: 97 [13] McCartney D G. Metall aams, 1988; 19A: 385 [14] Cornish A J. Met Set, 1975; 9: 477 [15] Sevier P E, Dore J E, Peterson W S. J Met, 1970; 22: 37 [16] Lee M S, Terry B S. Mater Set Technol, 1991; 7(7): 608 [17] Labarre L C, James R S, Witters J J. J Phes, 1987; 48(C3):93 [18] John D H St, Hogan L M. J Austral Inst Met, 1977; 22: 160 [19] Baner n A, Reihim M A, Reif W. Metallwiss Tech, 1985; 39:513 [20] Baeckerud L. UK Pat IS35957, 1971 [21] Guzowski M M, Senter D A, St~rth G K. UK Pat ApplGB 2162540A, 1986 [22] Reif W, Banerji A. UK Pat Appl GB 2171713A, 1986 [23] Sigworth G K. US Pat 5100488, 1992; 4873054, 1989;J812290, 1989 [24] Prasad K V S, Murty B S, Pramanik P, Mukunda P G,Chakraborty M. Mater Set Tech, 1996; 12. 766 [25] Adamkovicova K, Kosa L, Nerad i, Proks I, Strecko J. Ther-mochim Acta, 1995; 258: 15 [26] Thury W. Z Metallk, 1955; 46: 488 [27] Kattner U R, Lin J C, Chang Y A. Metall aams, 1992; 123A:2081 [28] Okamoto H. J Phase Equilibria, 1993, 14: 120 [29] Lee M S, Terry B S, Grieveson P. Metall Trans, 1993; 24B.955Q |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|