| RH法钢水定向循环流量操作模型的研究 |
| 区铁 刘建功 张捷宇 周文英 |
| 北京科技大学物理化学系;北京 100083 |
|
引用本文:
区铁; 刘建功; 张捷宇; 周文英 . RH法钢水定向循环流量操作模型的研究[J]. 金属学报, 1999, 35(4): 411-415 .
[1] Oeters F, translated by Ni R M, Zhang S B, Xiang C X.Metallurpy of Steelmaking. Beijing: Metallurgical Industry Press, 1997: 439(Oeters F 著;倪瑞明,张圣弼,项长祥译.钢冶金学.北京:冶金工业出版社,1997: 439) [2] Watanabe H, Asano K, Saeki T. Tetsu Hagals, 1968; 54:1327(渡透夫.浅野钢一,佐伯毅.铁钢,1968; 54: 1327) [3] Ono K, Yanagida M, Katoh T, Miwa M, Okamoto T.Denki-Seiko, 1981; 52: 149(小野清雄,柳田稔,加藤时夫,三轮守,冈本夫.电气制钢,1981; 52: 149) [4] Kuwabara T, Umezawa K, Mori K, Watanabe H. Trans IronSteel Inst Jpn,1988; 28: 305 [5] Xu K D, Fan Y Y, Li W P. SPeCial Steel, 1982; (5): 30(徐匡迪,攀养颐,李维平,特殊钢; (5): 30) [6] Ahn S B, Jung W G, Yim C H, Cheong K H, Kim Y H.Improvement Of RH Refining TeChnology for Pnduction ofUltra-Low Carbon Steel at Kwang Yang Works,POSCO.In: Steelmaking Conference Proceedings, Vol.80, Chicago:Iron & Steel Society, 1997: 123 [7] On T. Steelmaking, 1993; (1): 58(区铁.炼钢,1993; (1): 58) [8] Sumida N, Fujii T, Oguchi Y. Kawasaki Steel Ciho, 1983;15: 152(住田则夫,藤井也,小口征男.顺铁技报,1983; 15: 152) [9] Yu N W, Wei J H, Fan Y Y, Yang S L, Ma J C. J Northastern Unly, 1998; 19(Suppl.1): 118(郁能文,魏秀和,樊养颐,杨森龙,马金昌.东北大学学报,1998;19(增刊): 118) [10] Wang D L, Hong B Y. Vacuum Treatment of Molten Steel.Beijing: The Metallurgical industry Press, 1975: 96(王殿录,洪保义.钢液真空处理.北京:治金工业出版社,1975:96)% |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|