| 单晶镍基合金高温压缩蠕变的微观特征 |
| 田素贵 张静华 金涛 杨洪才 徐永波 胡壮麒 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳 110015 |
|
引用本文:
田素贵; 张静华; 金涛; 杨洪才; 徐永波; 胡壮麒 . 单晶镍基合金高温压缩蠕变的微观特征[J]. 金属学报, 1999, 35(4): 392-396 .
[1] Kear B H, Piearcey B J. Trans TMS AIMs 1967; 239: 1209 [2] Leverant G R, Kear B H. Metall Trans, 1970; 1: 491 [3] Takeuchi S, Kuramoto E. Acta Metall, 1973; 21: 415 [4] Courbon J, Ignat M, Louchet F. Acta Metall Mater, 1990;38: 663 [5] Kear B H, Wilsdorf H G F. aams TMS AIME, 1962; 224:382 [6] Par H, Saburi T, Nenno S. Scr Metall, 1976; 10: 1081 [7] Sun Y Q, Crimp M A, Hazzledine P M. Philos Mag, 1991,64: 223 [8] Hsiung L M, Stoloff N S. Acta Metall Mater, 1994; 42: 1457 [9] Ardell A J. Metall Trans,1985; A16: 2131 [10] Tian S G, Zhang J H, Yang H C, Xu Y B, Hu Z Q. MaterSet Technol, 1998; 14: 751 |
|