| 用NRTL方程预测三元,四元液态合金体系的热力学数据 |
| 侯怀宇 谢刚 |
| 昆明理工大学冶金系; 昆明 650093 |
|
引用本文:
侯怀宇; 谢刚 . 用NRTL方程预测三元,四元液态合金体系的热力学数据[J]. 金属学报, 1999, 35(3): 292-295 .
[1] Renon H, Prausnitz J M. AIChE J, 1968; 14: 135 [2] Hultgren R, Ors R L, Anderson P D, Kelley K K. SelectedValues of Thermodynamic Properties of Metals and Alloys,John Wiley & Sons, Inc., USA, 1963: 518, 552, 617, 629, 899 [3] John M. D, Robert D. P. Trans Metall Soc AIME, 1963; 227.1030 [4] Mellgren S. J Am Chem Soc, 1952; 74, 5037 [5] Elliott J F, Chipman J. J Am Chem Soc, 1951; 73: 2682 [6] Thompson W T, Leung A, Hurkot D G. Can Metall Q, 1973;12: 421 [7] Tassios D. Ind Eng Chem Process Des Dev. 1979; 18: 182 |
|