| 应用调制差示扫描量热计(Modulated-DSC)分离非晶态合金的玻璃化转变 |
| 吕昭平 李毅 黄思峻 冯元平 卢柯 |
| Department of Materials Science; National University of Singapore; Singapore 119260; |
|
引用本文:
吕昭平; 李毅; 黄思峻; 冯元平; 卢柯 . 应用调制差示扫描量热计(Modulated-DSC)分离非晶态合金的玻璃化转变[J]. 金属学报, 1999, 35(1): 73-77 .
| 1]ReadingM.TrendsPolymSci,1993;8:248[2]ReadingM,EliotD,HilVL.JThermAnal,40:949[3]O′ReilyKAQ,CantorB.ProcRSocLondon,1996;452A:2141[4]IshikiriyamaK,WunderlichB.Macromolecules,1997;30:4126[5]IshikiriyamaK,BolerA,WunderlichB.JThermAnal,1997;50(4):547[6]BolerA,SchichC,WunderlichB.ThermochimActa,1995;266:97[7]WagnerT,KasapSO.PhilosMag,1997;74B:667[8]GilPS,SauerbrunnSR,ReadingM.JThermAnal,1993;40:931[9]CahnRW,HaasenP.PhysicalMetalurgyrm.3thed,Amsterdam:North-HolandPhysics,1983:1826[10]InoueA,ChenS,MasumotoT.MaterSciEng,1994;179//180A:346[11]InoueA,ZhangT,TakeuchiA,ZhangW.MaterTransJIM,1997;37:636 |
|