| 快速加热和冷却法制备的极细多芯Nb_3A1线材的超导特性 |
| 毛大立;伊藤喜久男;和田仁 |
| 上海交通大学材料科学系国家教委高温材料及高温测试开放实验室;上海;200030;日本国立金属材料技术研究所;日本茨城县筑波;305;日本国立金属材料技术研究所;日本茨城县筑波;305 |
|
| CHARACTERIZATION OF A MULTIFILAMENTARY Nb3Al WIRE FABRICATED BY RAPIDLY HEATING AND RAPIDLY QUENCHING METHOD |
| MAO Dali(The Public Laboratory of State Education Commission for High Temperature Materials and High Temperature Tests; Department of Materials Science; Shanghai Jiaotong University; Shanghai 200030)ITOH Kihao;WADA Hitoshi(National Research Institute for Metals; Tsukuba; Ibaraki 305; Japan) |
引用本文:
毛大立;伊藤喜久男;和田仁. 快速加热和冷却法制备的极细多芯Nb_3A1线材的超导特性[J]. 金属学报, 1998, 34(7): 735-741.
,
,
.
CHARACTERIZATION OF A MULTIFILAMENTARY Nb3Al WIRE FABRICATED BY RAPIDLY HEATING AND RAPIDLY QUENCHING METHOD[J]. Acta Metall Sin, 1998, 34(7): 735-741.
1 Foner S, McNiff E J Jr, Geballe T H, Willens R H, Buehler E. Physica, 1971; 55: 534 2 Thirmr C L H, Pourralnimi S, Schwartz B B, Foner S. IEEE Trans Magn, 1985; MAG-21: 756 3 Yamada Y, Ayai N, Takahashi K, Sato K, Sugimoto M, Ando T, Takahashi Y, Nishi M. Adv Cryop Egg, 1994;40: 407 4 Inoue K, Iijima Y, Takeuchi T. Appl Phys Lett, 1988; 52: 1724 5 Takeuchi T, Iijima Y, Kosuge M, Kuroda T, Yuyama M, Inoue K. IEEE Trans Magn, 1989; MAG-25: 2068 6 Takeuchi T, Kosuge M, Iijima Y, Hasegawa A, Kiyoshi T, Inoue K. IEEE Trans Magn, 1991; MAG-27: 2045 7 Kuroda T, Wada H, Bray S L, Ekin J W. Fusion Eng Design, 1993; 20: 271 8 黑田恒生,和田仁日本金属学会志,1991;55:344(Kuroda T, Wada H J Jpn Inst Met, 1991; 55: 344) 9 Takeuchi T, Kuroda T, Itch K, Kosuge M, Iijima Y, Kiyoshi T, Matsumoto F, Inoue K. J Fusion Energy,1992; 11(1): 7 10黑田恒生,牛桐一宗,小高久男,汤山道也,和田仁,井上廉,罔田东一.日本原子力学会志,1995 37: 652(Kuroda T, Katagiri K, Kodafor H, Yuyama M, Wada H, Inoue K; Okada T.J At Enerpy Soc Jpn, 1995; 37: 652) 11 Kuroda T, Katagiri K, Kodaka H, Yuyama M, Wada H, Inoue K, Okada T. Physica,1996; B216: 230 12 Iijima Y, Kosuge M, Takeuchi T, Inoue K. Adv Cryop Eng, 1994; 40: 899 13 Iijima Y, Kosuge M, Takeuchi T, Inoue K. In: Haruyama T, Mitsui T, Yamafuji K eds., Proc 16th IntCryopenic Engineeriny Conf Int/Cryogenic Materials Conf Kitakyushu, Japan, Elsevier Science, 1996: 1697 14 Fukuda K, Iwaki G, Kimura M, Sakai S, Iijima Y, Takeuchi T, Inoue K, Kobayashi N, Watanabe K, Await S.In: Haruyama T, Mitsui T, Yamafuji K eds., Proc 16th Int Cryogenic Engineering/Conf Int CryogenicMaterials Conf Kitakyushu, Japan, Elsevier Science, 1996: 1669 15 Kramer E J. J Appl Phys, 1973; 44: 1360 16 Togano K, Takeuchi H, Tachikawa K. IEEE Trans Magn, 1983; MAG-19: 414 17 Takeuchi T, Togano T, Tachilera K. IEEE Trans Magn, 1987; MAG-23: 956 18 Clemente G, Habbal F, Tumbull D, Bevk J. Appl Phes Lett, 1985; 47: 640 19 Mueller D, Kehlenbeck M, Schaper W, Freyhart H C. Supereond Sci Technol Proc Conf 1991; 4: 365 20 Inoue K, Takeuchi T, Iijima L Y, Kosuge M. Cryogenics, 1989; 29: 361 |
|