| [011]多滑移取向铜单晶体的循环形变行为──Ⅱ.表面滑移特征及形变带 |
| 李小武;王中光;孙守光;吴世丁;李守新;李广义 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015;中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015;中国北方交通大学力学工程系;北京;100044;中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015;中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015;中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015 |
|
| CYCLIC DEFORMATION BEHAVIOR OF [011]MULTIPLE-SLIP-ORIENTED COPPER SINGLE CRYSTALS Ⅱ. Surface Slip Features and Deformation Bands |
| (LI Xiaowu; WANG Zhongguang; SUN Shouguang; WU Shiding; LI Shouxin;LI Guangyi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Mechanical Engineering; Northern Jiaotong University; Beijing 100044) |
引用本文:
李小武;王中光;孙守光;吴世丁;李守新;李广义. [011]多滑移取向铜单晶体的循环形变行为──Ⅱ.表面滑移特征及形变带[J]. 金属学报, 1998, 34(5): 552-560.
,
,
,
,
,
.
CYCLIC DEFORMATION BEHAVIOR OF [011]MULTIPLE-SLIP-ORIENTED COPPER SINGLE CRYSTALS Ⅱ. Surface Slip Features and Deformation Bands[J]. Acta Metall Sin, 1998, 34(5): 552-560.
1 Saletore M,Taggart R.Mater Sci Eng,1978;36:259 2 李小武,王中光,孙守光,吴世丁,李守新,李广义.金属学报,1998; 34:545(Li Xiaowu,Wang Zhangguang,Sun Shouguang,Wu Shiding,Li Shouxin .Li Guangyi.Acta Metall Sin,1998; 34:545) 3 Mughrabi H. Mater Sci Eng, 1978 33: 207 4 Gong B, Wang Z R, Wang Z G. Acta Mater, 1997 45: 1365 5 Barrett C S,Levenson L H.Trans Metall Soc AIME,1939;135:327 6 Barrett C S,Levenson L H.Trans Metall Soc AIME,1939;137:112 7 Honeycombe R K W. J Inst Met, 1951-1952 80: 45 8 Calnan E A.Acta Crystallogr,1952 ;5:557 9 Gostelow C R. Met Sci J, 1971;5: 177 10 Gong B, Wang Z G, Zhang Y W Mater Sci Eng, 1995; A194: 171 11 Li S X, Gong B, Wang Z G Scr Metall Mater, 1994 31: 1729 12 宫波,王中光,张轶伟,李广义,张天宜.金属学报,1994;30:439(Gong Bo, Wang Zhongguang, Zhang Yiwei, Li Guangyi, Zhang Tanyi. Acta Metall Sin, 1994 30: 439) 13 Vorren O, Ryum N Acta Metall, 1988; 36: 1443 14 Crocker A G, Abell J S、 Philos Mag, 1976 33: 305 15 Zhai T, Martin J W, Briggs G A D. Acta Metall Mater. 1995: 43: 3813 16 Zhai T, Martin J W, Briggs G A D, Wilkinson A J Acta Mater, 1996: 44: 3477 17 Suresh S.Fatigue of Materials London:Cambridge University Press,1991 18 Li X W, Hu Y M, Wang Z G Mater Sci Eng, 1998; in press 19 Reid C N. Deformation Geometry for Materials Scientists. Oxford: Pergamon Press, 1973 20 Villechaise P,Mendez J,Violan P. Acta Metall Mater,1991; 39:1683 |
|