| 锯齿状魏氏组织表面浮凸的扫描隧道显微镜研究 |
| 薄祥正;徐宁;方鸿生 |
| 清华大学材料科学与工程系;北京;100084;清华大学材料科学与工程系;北京;100084;清华大学材料科学与工程系;北京;100084 |
|
| STM STUDY ON THE SURFACE RELIEF EFFECTS ASSOCIATED WITH WIDMANSTAT SAWTEETH |
| BO Xiangzheng; XU Ning; FANG Hongsheng(Department of Materials Science and Engineering; Tsinghua University; Beijing 100084)Correspondent: BO Xiangzheng; Tel: (010)62782361; Fax: (010)62771160;E-mail. As -dms @m ailTsinghua. edu. cnManuscript received 1997-12-29; in revised form 1998-03-23 |
引用本文:
薄祥正;徐宁;方鸿生. 锯齿状魏氏组织表面浮凸的扫描隧道显微镜研究[J]. 金属学报, 1998, 34(12): 1249-1254.
,
,
.
STM STUDY ON THE SURFACE RELIEF EFFECTS ASSOCIATED WITH WIDMANSTAT SAWTEETH[J]. Acta Metall Sin, 1998, 34(12): 1249-1254.
1Dube C A, Aaronson HI, Mehl R F. Rev Met, 1958; 55: 20 2 Aaronson H I .In:Zackey V F.Aaronson H I.eds Decomposition of Austenite by Diffusional Processes.New York: Interscience Publishers, 1962: 387 3Aaronson H I.Laird C.Kinsman K R.Phase Transformations. Metals Park.Ohio:ASM,1970:313 4 Watson J D, McDougall P G. Acta Metall, 1973; 21: 961 5 Kinsman K R, Eichen E, Aaronson H I. Metall Trans. 1975; 6A: 303 6 hall M G, Aaronson H I.Metall Mater Trans ,1994; 25A: 1923 7薄样正,方鸿生,王家军,王峥华.金属学报,待发表(Bo X Z, Pang H S, Wang J J, Wang Z H. Acta Metall Sin.Accepted) 8 薄祥正,方鸿生 金属学报,待发表(BO X Z, Fang H S, Acta Metall Sin, Accepted) 9 Christian J W.In:Zackey V F,Aaronson H I eds:Decomposition of Austenite by Diffusional Proscesses. New York: Interscience, 1962: 371 10 Christian J W. Metall Mater Trans, 1994; 25A: 1821 11 Kurdjumow G V, Sachs G. Phwik Z, 1939; 64: 325 12 Binnig G, Rohrer H, Gerber Ch, WeibelE. Phys Rev Lett, 1982; 49: 57 13 Binnig G, ffehrer H. Snd SCi, 1983; 126: 236 14 Yamamoto M, Fujisawa T, Saburi T, Kurumisawa T, Kusao K. Surf Sci, 1992; 266: 289 15 Fang H S, Wang J J, Yang Z G, Li C M, Zheng Y K, Li C X. Metall Mater Trans,1996; 27A:1535 16 Wang J J, Fang H S, Zheng Y K, Yang Z G. ISIJ Int, 1995; 3s: 992 17 Yang Z G, Fang H S, Wang J J, Li C M. Zheng Y K. Phy Rev, 1995; B52: 7879 18 Swallow E,Bhadeshia H K D H.Mater Sci Technol.1996;12:121 19 Bo X z,Fang H S,Wang J J.Scr Metall.1997; 37:55s 20 Aaronson HI, Wells C. Trans AIME, 1956; 206: 1216 21 Aaronson HI, SPanos G, Masamura R A, Vardiman T G, Moon D W, Menon E S K, Hall M G. Mater SciEng,1995; B32:107 22 Wechsler M S, Lieberman D S, Read T A.J Met, 1953; 197: 1503 23 Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129 24 Wayman C M. Metallography, 1975; 8: 105 25 Spanos G,Hall M G,Metall Mater Trans.1996;27A:1519 |
|