Cu双晶的循环形变行为与疲劳裂纹萌生Ⅰ.循环形变行为和滑移形貌 |
胡运明;王中光 |
中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015;中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳;110015 |
|
CYCLIC DEFORMATION BEHAVIOR AND FATIGUE CRACK INIT1ATION IN COPPER BICRYSTALS |
I. Cyclic Deformation Behavior and Slip Morphology HU Yunming; WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy ofSciences; Shenyang 110015) (Manuscript received 1996-09- 12; in revised form 1997-03-07) |
引用本文:
胡运明;王中光. Cu双晶的循环形变行为与疲劳裂纹萌生Ⅰ.循环形变行为和滑移形貌[J]. 金属学报, 1997, 33(8): 814-823.
,
.
CYCLIC DEFORMATION BEHAVIOR AND FATIGUE CRACK INIT1ATION IN COPPER BICRYSTALS[J]. Acta Metall Sin, 1997, 33(8): 814-823.
1Suresh S著.王中光,于维成,臧启山等译.材料的疲劳.北京:国防工业出版社, 1993 2 Basinski Z S, Basinski S J. Prog Mater Sci, 1992; 26: 89 3 Mughrabi H. Mater Sci Eng,1978; A33: 207 4 Figueroa J C, Laird C. Acta Metall ,1981; 29:1679 5 Bhat S P, Laird C. Scr Metall,1978, 12: 687 6 Lukas P, Kunz L. Mater Sci Eng, 1985; A74: L1-L5 7 Liu C D, Massim M N, You D X. Acta Metall,1994; 42:1631 8 Mughrabi H. Scr Metall,1979; 13: 479 9 Polak J, Klesnil M. Mater Sci Enk,1984; 63:189 10胡运明,王中光.金属学报,1997;33:824 11 Cheng A S, Laird C. Mater Sci Eng, 1981; A51:55 12 Hook R E, Hirth J P. Actall Metall,1967;15: 535 13 Paider V, Pal P, Kadeckova S. ActaH Metall,1986; 34: 2277 |
|