| Pt_(69.0)Ni_(9.6)P_(21.4)合金的比热和Kauzmann温度 |
| 蒋青;徐晓亚;李建忱 |
| 吉林工业大学;长春;130025;吉林工业大学;长春;130025;吉林工业大学;长春;130025 |
|
| SPECIFIC HEAT AND KAUZMANN TEMPERATURE OF PtNiP ALLOY |
| JIANG Qing;XU Xiaoya; Li Jianchen (Jilin University of Technology; Changchun130025) |
引用本文:
蒋青;徐晓亚;李建忱. Pt_(69.0)Ni_(9.6)P_(21.4)合金的比热和Kauzmann温度[J]. 金属学报, 1997, 33(6): 660-666.
,
,
.
SPECIFIC HEAT AND KAUZMANN TEMPERATURE OF PtNiP ALLOY[J]. Acta Metall Sin, 1997, 33(6): 660-666.
1Johnson W L.Prog Mater Sci,1986;30:81 2Fecht H J.Johnson W L. Nalure, 1988; 334: 50 3Cahn W. Nature, 1986: 323: 668 4 Kauzmann W. Chem Rev, 1948; 43: 219 5 Wolf D,Okamoto P R,Yip S,Lutsko J F,Kluge M.J Mater Res.1990;5:286 6 fecht H J. Nature, 1992; 356: 133 7 Chen H S.J Non-Cryst Solids,1973:12:333 8Inoue A,Zhang T,Masumoto T.JNon-Cryst Solids,1993-156-158:473 9 Chen H S.Acta Metall.1974;22:1505 10 Jiang Q,Li J C,Tong J.Mater Sci Eng,1995;A196,165 11卢柯.金属学报,1992;28:B17 12Bergman C, Komarek K L. Calphad, 1985; 9(1): 1 13 Agren J,Cheynet B.Clavaguera-Mora M T,Hack K,Hertz J,Sommer F,Kattner U.Calphad,1995:19:449 14蒋青,徐晓亚,赵明.金属学报,1997;33待发表 15 Saslow W S Phys Rev B, 1988; 37: 676 16 Bruning R,Samwer K.Phys Rev B,1992;46:11318 17 Klose G、Fecht J H.Mater Sci Eng,1994;A179/180:77) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|