| 薄板坯连铸结晶器内钢液流场电磁制动的模拟研究 |
| 李宝宽;赫冀成;贾光霖;高允彦 |
| 东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006 |
|
| ELECTROMAGNETIC BRAKING ON FLOW FIELD OF MOLTEN STEEL IN THE THIN-SLAB CONTINUOUS CASTING MOLD |
| LI Baokuan;HE Jicheng;JIA Guanglin;GAO Yunyan(Northeastern University; Shenyang 110006) |
引用本文:
李宝宽;赫冀成;贾光霖;高允彦. 薄板坯连铸结晶器内钢液流场电磁制动的模拟研究[J]. 金属学报, 1997, 33(11): 1207-1214.
,
,
,
.
ELECTROMAGNETIC BRAKING ON FLOW FIELD OF MOLTEN STEEL IN THE THIN-SLAB CONTINUOUS CASTING MOLD[J]. Acta Metall Sin, 1997, 33(11): 1207-1214.
1NagaiJ.IronSteelEny,1984;61:41 2IsizukaH,YamadaS,OhnishiM.CAMP—ISIJ,1989;2:298 3ZezeM,HaradaH,TakeuchiE,IshiiT.Proc76thSteelmakingConf,Warrendale,PA:IronandSteelSociety,1993:267 4KariyaK,KitanoY,KugaM,IdogawaA,SorimachiK.Proc77thSteelmakingConf,Warrendale,PA:IronandSteelSociety,1994:53 5ZezeM,HaradaH,TakeuchiE,IshiiT.Proc79thSteelmakingConf,Abstract,Warrendale,PA:IronandSteelSociety,1996 6JonesWP,LaunderBE.IntJHeatMassTransfer,1973;16:1119 7周波.冶金工业部钢铁研究总院硕士学位论文,1995 |
|