金属Co超细粉的γ射线辐照制备
陈祖耀;张国春;朱玉瑞
中国科学技术大学结构研究开放实验室;合肥230026;中国科学技术大学结构研究开放实验室;合肥230026;中国科学技术大学结构研究开放实验室;合肥230026
PREPARATION OF NANOCRYSTALLINE METALLIC α-Co BY γ-RAY RADIATION
CHEN Zuyao; ZHANG Guochun;ZHU Yurui (Structure Research Laboralory; Science & Technology of China; Chinese academy of Sciences; Hefei 230026)
引用本文:

陈祖耀;张国春;朱玉瑞. 金属Co超细粉的γ射线辐照制备[J]. 金属学报, 1997, 33(10): 1110-1114.
, , . PREPARATION OF NANOCRYSTALLINE METALLIC α-Co BY γ-RAY RADIATION[J]. Acta Metall Sin, 1997, 33(10): 1110-1114.

全文: PDF(1744 KB)  
摘要: 采用γ射线辐照可溶性Co盐溶液可制备金属Co超细微粒及其相应粉体.X射线衍射、电子衍射及相应的TEM形貌分析表明,金属粒子呈现各向异性生长的结晶体,当用醋酸Co作为出发原料,被辐照溶液浓度在0.005-0.2mol/L的范围内,辐照剂量和pH分别在2.3×104-3.9×105Gy和6.0-10.0时,超细粒子的平均粒径一般都在30nm左右.
关键词 金属Co超细粉γ射线辐照微波辐照    
Abstract:Ultrafine particles and powders of metallic α-Co were prepared in an aqueous solution of Co2+ by γ-ray radiation. The ultrafines appear as nanocrystallined particles according to X-ray and electron diffraction. The average size of particles is 30 nm while concentration of cobalt acetate solution, irradiation dose and solution pH are in the range of 0.005-0.2 mol / L, 2.3×104-3.9 ×105 Gy and 6.0-10.0 respectively.
Key wordsα-Co ultrafine particle    γ-ray radiation    microwave radiation
收稿日期: 1997-10-18     
基金资助:国家自然科学基金!59572031
1 Gibson C P,Putzer K J,Science,1995;267:1338
2 Haneda K.Can J Phys,1987;65:1233
3 Lion H.Chien C L.J appl Phys, 1988;63:4240
4 Bridger K, Watts J, Chien C L,J appl Phys, 1988;63:3233
5 Harriman a Pickering I J, Thomas J M, Christensen P a.J Chem Soc Faraday Trans,1988;1842795
6罗红梅.中国科学技术大学硕士学位论文,1994
7 Xiao J Q.Jiang J S ,Chien C L,Phys Rev Lett,1992;68:3749
8 Tsoukatos a,Wan H,Hadijipanayis G C,Li Z G.appl Phys Lett,1992;61:3059
9 Chen J P,Lee K M.J appl Phys,1994;75:5876
10 Chow G M,Kurihara L K,Kemner K M,Schoen P E,Elam W T、J Mater Res;1995;10:1546
11 Vasilikov a Y,olenin a Y,Titova E F,Sergeev V a.J Colloid Inter face Sci,1995;169:356
12 Jin Gu,Zhu Yu-rui,jiang Wan-quan.Submitted to analyst
13张曼维编著,辐射化学入门,合肥:中国科学技术大学出版社,1993
14张国春,陈祖耀,朱玉瑞等,硅酸盐学报(待发表)
15 Katsumura Y, Jiang P Y,Nagaishi R, J Phvs Chem,1991:95:4435
16陈祖耀,陈波,钱逸泰,张曼维,杨丽、范成高.金属学报1992;28:B169
[1] 陈祖耀;陈■;朱玉瑞;陈文明;钱逸泰;杨丽. 紫外射线辐照制备Cu_2O超细粉及其宏观动力学[J]. 金属学报, 1997, 33(3): 330-336.
[2] 朱英杰;钱逸泰;张曼维;陈祖耀. γ射线辐照-水热处理法制备纳米金属粉末[J]. 金属学报, 1994, 30(18): 259-264.
[3] 张桂林;徐峰;刘文宏;俞方华;王景成;邵自昌. γ辐照对CuZnAl形状记忆合金影响的研究[J]. 金属学报, 1992, 28(3): 42-44.