| Ni-Ti-Nb宽滞后形状记忆合金的形变诱发马氏体相变及其可逆性 |
| 赵连城;蔡伟 |
| 哈尔滨工业大学;哈尔滨;150001;哈尔滨工业大学;哈尔滨;150001 |
|
| DEFORMATION-INDUCED MARTENSITIC TRANSFORMATION AND ITS REVERSIBILITY IN Ni-Ti-Nb WIDE HYSTERESIS SHAPE MEMORY ALLOYS |
| ZHAO Liancheng; CAI Wei (Harbin Institute of Technology; Harbin 150001) |
引用本文:
赵连城;蔡伟. Ni-Ti-Nb宽滞后形状记忆合金的形变诱发马氏体相变及其可逆性[J]. 金属学报, 1997, 33(1): 90-98.
,
.
DEFORMATION-INDUCED MARTENSITIC TRANSFORMATION AND ITS REVERSIBILITY IN Ni-Ti-Nb WIDE HYSTERESIS SHAPE MEMORY ALLOYS[J]. Acta Metall Sin, 1997, 33(1): 90-98.
1Melton K N,Proft J L,Duerig T W.Proc of the M R S Int Meeting on Advanced Materials Vol.9,1988:165 2 Zhao L C,Duerlg T W,Wayman C M.Proc of the M R S Int Meeting on Advanced Materiak,Vol.9,1988:171 3Zhao L C,Duerig T W, Just S,Melton K N,Proft J L,Yu W,Wayman C M Scr Metall 1990;24:221 4 Cai W,Zhang C S Zhao L C J Mater Sci Lett,1994;13:8 5Zhang C S, Zhao L C,Duerig T W,Wayman C M Scr Metall, 1990;24:1807 6 Zhao L C,Zhang C S Proc of the ICOMAT-92 1993:947 7Zhao L C,Zhang C S Cai W Proc of the SMM‘94,1994:225 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|