Please wait a minute...
金属学报  1997, Vol. 33 Issue (1): 22-28    
  论文 本期目录 | 过刊浏览 |
试论我国解放后炼铁技术路线
张寿荣
武汉钢铁公司;武汉;430083
EVALUATION OF TECHNOLOGICAL POLICY OF IRONMAKING IN CHINA
ZHANG Shourong (Wuhan Iron and Steel Corporation; Wuhan 430083)
引用本文:

张寿荣. 试论我国解放后炼铁技术路线[J]. 金属学报, 1997, 33(1): 22-28.
. EVALUATION OF TECHNOLOGICAL POLICY OF IRONMAKING IN CHINA[J]. Acta Metall Sin, 1997, 33(1): 22-28.

全文: PDF(826 KB)  
摘要: 本文简要回顾建国以来我国炼铁技术路线的演变过程,并展望周世纪的前景
关键词 : 中国炼铁技术路线,  回顾    
Abstract:This paper briefly reviews the evaluation of technological policy of ironmaking in China after the founding of People's Republic and forecasts the prospect in the 21st century.
Key words: technological policy of ironmaking in China    review