催化还原碳钛磁铁矿反应动力学
兰尧中;刘纯鹏
云南师范大学;昆明工学院
KINETICS OF CARBON CATALYTIC REDUCTION OF TITANOMAGNETITE CONCENTRATE
LAN Yaozhong(Yunnan Normal University; Kunming 650092); LIU Chunpeng(Kunming Institute of Technology; Kunming 650092)(Manuscript received 1995-09-12)
引用本文:

兰尧中;刘纯鹏. 催化还原碳钛磁铁矿反应动力学[J]. 金属学报, 1996, 32(5): 502-503.
, . KINETICS OF CARBON CATALYTIC REDUCTION OF TITANOMAGNETITE CONCENTRATE[J]. Acta Metall Sin, 1996, 32(5): 502-503.

全文: PDF(136 KB)  
摘要: 本文借助于热重分析法,测定钛磁铁矿碳热还原动力学。试验结果表明,添加碱金属碳酸盐能够加速钛磁铁矿碳热还原反应。催化作用顺序Na_2CO_3>Li_2CO_3
关键词 : 钛磁铁矿,  碳还原,  碱金属碳酸盐,  催化反应动力学    
Abstract:Catalytic kinetics of the carbothermic reduction of titanomagnetite concentrate was examined in the temperature range from 900 to 1150℃ . An addition of alkali carbonate enhances the rate of the reduction of titanomagnetite, the catalytic effects are in the order: Na_2CO_3 > Li_2CO_3.
Key words: titanomagnetite carbon reduction    alkali metal carbonate    catalytic kinetics.
收稿日期: 1996-05-18     
[1] 刘清才. 钒钛磁铁矿熔态还原速度与渣相结构的关系[J]. 金属学报, 1996, 32(10): 1081-1086.
[2] 张丙怀;刘清才;李长伟;邹德余;孙锦彪. 钒钛磁铁矿熔融还原渣系中钒还原的热力学规律[J]. 金属学报, 1993, 29(5): 49-55.
[3] 张丙怀;邹德余;金克和;刘清才. 钒钛磁铁矿熔融还原速度研究[J]. 金属学报, 1992, 28(1): 51-56.