球磨能量对Mo-Si混合粉末机械合金化的影响
柳林;秦勇
中国科学院固体物理研究所
EFFECT OF MILLING ENERGY ON MECHANICAL ALLOYING OF Mo-Si POWDER MIXTURE
LIU Lin; QIN Yong(Institute of Solid Stale Physics; Chinese Academy of Sciences;Hefei 230031) (Manuscript received 1995-06-27; in revised form 1995-11-27)
引用本文:

柳林;秦勇. 球磨能量对Mo-Si混合粉末机械合金化的影响[J]. 金属学报, 1996, 32(4): 423-428.
, . EFFECT OF MILLING ENERGY ON MECHANICAL ALLOYING OF Mo-Si POWDER MIXTURE[J]. Acta Metall Sin, 1996, 32(4): 423-428.

全文: PDF(443 KB)  
摘要: 利用X射线衍射,SEM和TEM研究了Mo-Si(原子比为1:2)混合粉末在不同球磨条件下的机械合金化过程.Mo/Si相变与球磨强度密切相关,高能球磨有利于稳定相α-MoSi_2的形成,而低能球磨有利于亚稳相β-MoSi_2的形成。对不同球磨条件下的相变动力学和热力学进行了讨论.
关键词 : Mo/Si相变,  球磨能量,  α-MoSi_2,  β-MoSi_2    
Abstract:The mechanical alloying of Mo-Si powder mixture with atomic ratio of 1:2 under different milling conditions has been studied by means of X-ray diffractometry (XRD), SEM and TEM. It is found that the higher energy milling favours the formation of stable α-MoSi_2, while the lower energy milling promotes the formation of metastable β-MoSi2. Thermodynamics and kinetics aspects related to the different phase transformations have been discussed. Correspondent: QIN Yong,(senior engineer, Institute of Solid State Physics, Chinese Academy of Sciences, Hefei 230031)
Key words: Mo/Si reaction    milling energy    α-MoSi_2    β-MoSi_2
收稿日期: 1996-04-18     
1KochCC,CavinOB,McKamcyCG,ScarbroughJO.ApplPhysLett,1983:43:10172FechtNJ,HanG,FuZ,JohnsonWL.JApplPhys,1990;67:17443EchertJ,SchultzL,UrbanK.ZMetallk,1990;81:8624SchultzL,WeckerJ,HellsternE.JApplPhys,1987;61:38535LiuL,DongYD.NanostructMater,1993;2:4636LiuL,PadellaF,GuoW,MaginiM.ActaMetallMater,1995;43:37557SchwarzRB,SrinivasanSR,PetrovicJJ,MaggioreCJ.MaterSciEng,1992;A155:758MaE,PaganJ,GranfordG,AtzmonMJMaterRes,1993;8.18369MarquardDW.JSocIndApplMath,1963;91:43110MaginiM,CollelaC,GuoW,IasonnaA,MartelliS,PadellaF.IntJMechanochemMechAlloying,1994;1:1411MaginiM.MaterSciFor,1992;88-90:12112BurgioN,IasonnaA,MaginiM,MartelliS,PadellaF.ILNuovoCimento,1991;13D:45913MauriceDR,CourtenyTH.MelallTrans,1990;21A:28914AbdellaouiM,GaffetE.JAlloysCompo,1994;209:35115DolandCM,NemanichRJ.JMaterRes,1990;5:2854