金属学报  1996, Vol. 32 Issue (4): 393-396    
  论文 本期目录 | 过刊浏览 |
硼铁矿冶炼Fe-Si-B合金的工艺研究
刘素兰;张显鹏;崔传孟
东北大学
METALLURGICAL STUDY ON Fe-Si-B ALLOY FROM LIAONING LUDWIGITE
LIU Sulan; ZHANG Xianpeng; CUI Chuanmeng(Northeastern University; Shenyang 110006)(Manuscript received 1995-06-16; in revised form 1995-11-28)
引用本文:

刘素兰;张显鹏;崔传孟. 硼铁矿冶炼Fe-Si-B合金的工艺研究[J]. 金属学报, 1996, 32(4): 393-396.
, , . METALLURGICAL STUDY ON Fe-Si-B ALLOY FROM LIAONING LUDWIGITE[J]. Acta Metall Sin, 1996, 32(4): 393-396.

全文: PDF(231 KB)  
摘要: 建立了以辽东硼铁矿为原料,用碳热还原成碳-铝热还原冶炼Fe-Si-B合金的工艺,测定了还原时间和温度对合金中B,Si,C含量的影响以及C含量与B和Bi含量的关系:用熔渣-金属平衡方法对合金进行脱Al,研究了碱度以及B2O3和SiO2含量对合金中Al含量的影响.结果表明,该工艺可使合金中C含量降至0.15%,Al含量小于0.05%.
关键词 : 硼铁矿,  碳热还原,  铝热还原,  Fe-Si-B合金    
Abstract:Fe-Si-B alloy has been produced from the Liaoning ludwigite by carbothermic or carbon-aluminothermic method. The effects of reducing time and temperature on B, Si and C contents in melt were investigated, and the relationship between C content and B and Si contents in melt was also discussed. The residual AI in melt was excluded by means of slag-metal equilibrium method, and the variations of Al content in melt with basicity and B and Si oxides were determined. The experimental results showed that it is feasible to produce Fe-Si-B alloy from Liaoning ludwigite and C and Al in alloy can be controlled down 0. 15% and 0.05% respectively.Correspondent: LIU Sulan, associate professor, P.O. Box 119, (Northeastern University, Shenyang 110006)
Key words: ludwigite    carbothermic    aluminothermic    Fe-Si-B alloy
收稿日期: 1996-04-18     
1SussmanRC,EvansLG.MetallTrans,1987;18B,712鱼谷进,铃木邦辉.日本公开特许公报,昭59-118853,19843SinghalSC.USPat,4602948,19864邹元,张子青,田彦文,周继程,汪光裕.中国专利,CN1050046A,19915俞荣祥,刘素兰,冀春林.钢铁,1987;22:86梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:508
[1] 戴文斌 王新丽 于景坤 邹宗树. 碳热还原氮化法合成MgAlON[J]. 金属学报, 2011, 47(11): 1440-1444.
[2] 马北越; 于景坤; 孙勇 . ZrO2--SiC复合材料的合成及其添加对Al2O3-C质耐火材料抗氧化性能的影响[J]. 金属学报, 2007, 43(10): 1059-1064 .
[3] 于金; 蒋建清; 方峰; 董岩; 谈荣生; 吴三械 . 真空铝热还原法制备金属Sr的热力学分析及实验研究[J]. 金属学报, 2005, 41(8): 824-828 .
[4] 徐桂英;李建保;谢志鹏;黄勇. NbC_x晶须的制备[J]. 金属学报, 1998, 34(2): 205-210.
[5] 刘兵海;欧阳世翕;张跃. 微波碳热还原法制备TiN[J]. 金属学报, 1996, 32(9): 921-925.
[6] 官可洪;王军. 非晶态Fe_(1-x)(Si,B)_x合金的内禀磁性和磁各向异性[J]. 金属学报, 1989, 25(5): 111-114.