金属学报  1996, Vol. 32 Issue (2): 219-224    
  论文 本期目录 | 过刊浏览 |
XPS数据处理的曲线拟合组合算法及检验
龚沿东
中国科学院金属研究所
COMBINATION ALGORITHM FOR CURVE FITTING OF XPS DATA AND DETECTION
GONG Yandong(Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-06-12)
引用本文:

龚沿东. XPS数据处理的曲线拟合组合算法及检验[J]. 金属学报, 1996, 32(2): 219-224.
. COMBINATION ALGORITHM FOR CURVE FITTING OF XPS DATA AND DETECTION[J]. Acta Metall Sin, 1996, 32(2): 219-224.

全文: PDF(364 KB)  
摘要: 本文针对XPS(X射线光电子能谱)数据处理中线型选择的问题作出了一个新改进,在曲线拟合过程中应用了一个卷积线型。新算法被称为"组合算法"对Cu标样3p谱和Fe-Mn-Al合金钝化膜Ols谱的拟合表明,它比选择Gauss-Lorentz积函数(GLP)或Gauss-Lorentz和函数(GLS)更为准确和有效
关键词 : XPS,  XPS线型,  组合算法    
Abstract:A new line shape was chosen for curve fitting of XPS (X-ray photoelectron spectroscopy) data. In general. the GLP(Gauss-Lorentz product function) orGLS(Gauss-Lorentz sum function) was used as the line shape of XPS, but they are not strict because the true line shape is a convolution of many comments. A convoluted line shape is chosen in fitting procedure. The new algorithm is called ‘combination algorithm' . A detec tion was taken with Cu 3p spectrum and O ls spectra of Fe-Mn-Al alloy. It is shown that the combination algorithm is more effective for the process of XPS data than GLP and GLS.(Correspondent: GONG Yandong, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110015)
Key words: XPS    line shape of XPS    combination algorithm
收稿日期: 1996-02-18     
1SherwoodPMA.PracticalSurfaceAnalysis,2nded.,Chechester:JohnWileyandSons,1990;1:5552SherwoodPMA.PracticalSurfaceAnalysisbyAugerandX-ray,photoelectronSpectroscopy,Chechester:JohnWileyandSons,1983:4453ShirleyDA.PhysRev,1972;B5:4709
[1] 宋贵宏,李贵鹏,刘倩男,杜昊,胡方. 溅射沉积Mg2(Sn, Si)薄膜组织结构与导电性能[J]. 金属学报, 2019, 55(11): 1469-1476.
[2] 李付绍 安茂忠 刘光洲 段东霞. 硫酸盐还原菌对18--8不锈钢点蚀行为的影响[J]. 金属学报, 2009, 45(5): 536-540.
[3] 朱逢吾; 于广华; 李明华; 姜宏伟; 赖武彦 . 插入Bi层对NiFe/Cu/NiFe/FeMn自旋阀多层膜交换耦合的影响[J]. 金属学报, 2002, 38(6): 617-620 .
[4] 关山; 张琦 . 利用XPS及电化学方法研究电镀Cr添加剂的作用机理[J]. 金属学报, 2000, 36(11): 1179-1182 .
[5] 谢天生; 戴贵平; 成会明; 范兆忠; 叶恒强 . 高定向石墨表面激光溅射硼及超结构的扫描隧道显微镜观察[J]. 金属学报, 1999, 35(7): 685-688 .
[6] 安础;黑祖昆;岡部芳雄;岩木正哉. 纯铁表面Ti~+-O~+二重离子注入后着色的研究[J]. 金属学报, 1995, 31(15): 116-122.