Please wait a minute...
金属学报  1996, Vol. 32 Issue (2): 211-214    
  论文 本期目录 | 过刊浏览 |
纳米微晶软磁合金中的磁织构
刘涛;徐祖雄;翟启华;马如璋;罗彤;张传历
北京科技大学;冶金工业部钢铁研究总院;北京科技大学材料物理系
MAGNETIC TEXTURE IN NANOCRYSTALLINESOFT MAGNETIC ALLOY
LIU Tao; XU Zuxiong; ZHAI Qihua; MA Ruzhang(University of Science and Technology Beijng; Beijing 100083) LUO Tong; ZHANG Chuanli(General Research Institute of Iron and Steel; Ministry of Metallurgicl Industry; Beijing 100081)(Manuscript received 1995-05-22; in revised form 1995-10-27)
引用本文:

刘涛;徐祖雄;翟启华;马如璋;罗彤;张传历. 纳米微晶软磁合金中的磁织构[J]. 金属学报, 1996, 32(2): 211-214.
, , , , , . MAGNETIC TEXTURE IN NANOCRYSTALLINESOFT MAGNETIC ALLOY[J]. Acta Metall Sin, 1996, 32(2): 211-214.

全文: PDF(316 KB)  
摘要: 用M ssbauer谱方法研究了超微晶软磁合金中存在的磁织构现象,对测与未测过磁性的两组不同温度下退火的Fe_(73.5)Cu_1Nb_3Si_(13.5)B_9合金的测量结果表明,晶化以后在非晶条带平面内出现了明显的沿带长轴择优取向的宽畴成分,这种磁织构现象可能是非晶条带的形状效应造成的,并非磁测量的扰动结果。
关键词 : M ssbauer谱,  超微晶软磁合金,  磁织构    
Abstract:Mossbauer spectroscopy was employed to investigate the magnetic texture in The nanocrystalline soft magnetic alloy Fe_(73.5)Cu_1Nb_3Si_(13.5)B_9. After crystallization a wide magnetic domain appeared obviously, which oriented preferently along the long axis of the ribbon plane and may be associated with the shape effect of the ribbon sample.(Correspondent: LIU Tao, Department of Materials Physics, University of Science and Technology Beijing,Beijing 100083)
Key words: M ssbauer spectrum    nanocrystalline soft magnetic alloy    magnetic texture
收稿日期: 1996-02-18     
1YoshizawaY,OgumaS,YamauchiK.JApplPhys,1988;64:60442马如璋.穆斯堡尔谱学,北京钢铁学院,19843徐祖雄,马如璋,平爵云.中国科学,1985;A(1):444徐祖雄,许震东,杨会生,马如璋.科学通报,1993;38:5125StearsMB.PhysRev,1963;129:11366LiuT,zhaoZT,XuZX,MaRZ,GuoYH,CaoHM,wangYY.JApplPhys,1995;77:62147JiangJ,AubertinF,GonserU,HilzingerH-R.ZMetallk,1991;82:6988PundtA,HampelG,HesseJ.ZPhys.1992;B87:659BOHCOBCКИЙCB,著,寥莹译.铁磁学,北京:科学出版社,1965:34210HerzerG.IEEETransMagn,1990:26:139711ZbroszczykJ,CiurzynskaC,WyslockiB.JMagnMagnMater,1994;133:34712HiragaK,KohmotoO.MaterTransJIM,1991;33:86813SchaferR,HubertA,HerzerG.JApplPhys,1991;69:53252
[1] 王魁香;郝兆印;邓京川;刘密兰;陆国会. 四种铁基合金的M■ssbauer谱研究[J]. 金属学报, 1996, 32(5): 469-473.
[2] 马如璋;刘涛;陈菊芳;杨国斌;徐祖雄;顾红霞. 钇对超微晶软磁合金结构和磁性能的影响[J]. 金属学报, 1996, 32(2): 207-210.