氧化铝生产中“硅渣”的组成和结构研究
邓红梅;曾文明;陈念贻
中国科学院上海冶金研究所
COMPOSITION AND CRYSTAL STRUCTURE OF Na-Al SILICATE SLIME IN ALUMINA PRODUCTION
DENG Hongmei;ZENG Wenming;CHEN Hianyi (Shanghai Institute of Metallurgy;Chinese Academy of Sciences;Shanghai 200050)(Manuscript received 1995-10-23; in revised form 1996-08-26)
引用本文:

邓红梅;曾文明;陈念贻. 氧化铝生产中“硅渣”的组成和结构研究[J]. 金属学报, 1996, 32(12): 1248-1251.
, , . COMPOSITION AND CRYSTAL STRUCTURE OF Na-Al SILICATE SLIME IN ALUMINA PRODUCTION[J]. Acta Metall Sin, 1996, 32(12): 1248-1251.

全文: PDF(290 KB)  
摘要: 综合运用X射线衍射、红外光谱、差热分析等方法,研究氧化铝生产中脱Si反应生成物--水合铝硅酸钠渣(硅渣)的组成和结构,证明其为有硅原子缺位的羟基方钠石,SiO_2与Al_2O_3摩尔比小于2.0主要系方钠石晶格骨架上硅原子缺位所致.
关键词 : 硅渣,  羟基方钠石,  Si原子缺位    
Abstract:The composition and crystal structure of the" White mud" ,or the Na-Al silicate slime in alumina production, is investigated by X-ray diffraction,IR spectra,differential thermal analysis, density detemination and chemical analysis concurrently. The chief phase, containing sodium aluminosilicate hydrate, has been identified to be hydroxy-sodalite crystals, usually having defect structure with vacancies of silicon atoms on the skeleton of sodalite lattice.
Key words: Na-Al silicate slime    hydroxy-sodalite    silicon atom vacancy
    