恒温超塑焊接接头断口分析 |
杨蕴林;李志;李炎 |
洛阳工学院 |
|
FRACTURE ANALYSIS OF JOINT AFTER CONSTANT TEMPERATURE SUPERPLASTIC WELDING |
YA NG Yunlin; LI Zhi; LI Yan(LuoYang institute of TechnoLogy); Luoyang 471039)(Manuscript received 1994-08-31; in revised form 1995-03-31) |
引用本文:
杨蕴林;李志;李炎. 恒温超塑焊接接头断口分析[J]. 金属学报, 1995, 31(20): 384-38.
,
,
.
FRACTURE ANALYSIS OF JOINT AFTER CONSTANT TEMPERATURE SUPERPLASTIC WELDING[J]. Acta Metall Sin, 1995, 31(20): 384-38.
1THXOHOBAC著,刘春林译.金属与合金的超塑性效应.北京:科学出版社,1983:110,852超塑性研究会编,康达昌等译.超塑性与金属加工技术.北京:机械工业出版社,1985:1883刘晓夷.钢的恒温超塑性压接的研究,洛阳工学院硕士学位论文,19914Ka3aKobHφ著,何康生等译.材料的扩散焊接.北京:国防工业出版社,1984:23 |
|