| 熔滴冲击下MIG焊接熔池的计算机模拟 |
| 曹振宁;武传松;吴林 |
| 山东工业大学;哈尔滨工业大学 |
|
| COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT |
| CAO Zhenning(Shandong Polytechnic Unversity; Jinan);WU Chuansong; WU Lin (Harbin Institute of Technology) |
引用本文:
曹振宁;武传松;吴林. 熔滴冲击下MIG焊接熔池的计算机模拟[J]. 金属学报, 1994, 30(24): 537-542.
,
,
.
COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT[J]. Acta Metall Sin, 1994, 30(24): 537-542.
| 1PadoE,WeckamnDC.MetallTrans,1989;20B:9372TsaoKC,WuCS.WeldJ,1988;67:70-s3武传松,吴林,陈定华.焊接学报,1991;12:1894ChooRTC,MukaiK,ToguriJM.WeldJ,1992;71:139-s5EssersWG,WalterR.WesdJ,1981;60:37-s6武传松,曹振宁,吴林.金属学报,1992;28:B4277KouS,WangYH.WeldJ1986;65:63-s8WoodsRA.WeldJ,1971;50:163-s9HeipleCR,RoperJR.Weld,1982;61:97-s |
|