金属学报  1994, Vol. 30 Issue (17): 238-242    
  论文 本期目录 | 过刊浏览 |
SrCeO_3基高温质子导体及Al液定氢探头
郑敏辉;陈祥
北京科技大学
SrCeO_3 BASED HIGH TEMPERATURE PROTON CONDUCTOR AND HYDROGEN PROBE
ZHENG Minhui; CHEN Xiang (University of Science and Technology Beijing)
引用本文:

郑敏辉;陈祥. SrCeO_3基高温质子导体及Al液定氢探头[J]. 金属学报, 1994, 30(17): 238-242.
, . SrCeO_3 BASED HIGH TEMPERATURE PROTON CONDUCTOR AND HYDROGEN PROBE[J]. Acta Metall Sin, 1994, 30(17): 238-242.

全文: PDF(318 KB)  
摘要: 以自制成分为SrCe_(0.95)Yb_(0.05)O_(3-α)的致密陶瓷管为固体电解质,以Ca/CaH2混合物为参比物组装氢探头。探头插入Al液构成氢浓差电化学电池:Mo,Ca/CaH_2|H ̄+conductor|[H]moltenAl’Mo对高氢含量Al液进行测定,电动势稳定时间长达1.8ks,准确反映了氢过饱和度.用六氯乙烷脱氢处理时电动势也有迅速正确的响应。使用后的固体电解质经X射线衍射未测出相变化。热重分析表明让SrCeO3基陶瓷中Sr过量可减轻其中4价Ce离子被还原程度。
关键词 : SrCeO_3,  质子导体,  定氢探头,  铝液    
Abstract:Hydrogen probes were constructed with highly dense tubes of SrCe0.95Yb0.05O3-α based proton conductor made by the authors, and with the mixture of Ca/CaH2. By insertion of the probe into liquid Al sample, the hydrogen concentration cell: Mo, Ca/CaH2|H+conductor[H]molten Al, Mo, is available to determine its hydrogen content. EMF of the probe was stable for 1.8 ks and also responded rapidly and accurately to the dehydrogenation by hexachloroethane. XRD and TG analysis of the recovered proton conductor showed that no other phase but perovskite was identified and the excess of Sr improves the stabiltiy of the proton conductor under strong reducing atmosphere.
Key words: StCeO_3    proton conductor    hydrogen probe    liquid Al
    
基金资助:国家自然科学基金
1北村照夫.铁匕钢,1989:75:3962GeeR,FrayDJ.Metall,Trans,1978;9B:4273IwaharaH,EsakaT,UchidaH,MaedaN.SolidStateIonics,1981;3//4:3594矢岛保,岩原弘育,武津典彦,大桥照男,小出邦博.轻金属,1992;263:425郑敏辉,甄秀欣,马淑云.第四届全国高技术陶瓷学术年会论文集,1992,4396甄秀欣,郑敏辉,第四届全国高技术陶瓷学术年会论文集,1992,4427ZhengM,ZhenX.SolidStateIonics,1993;59:1678ZhengM,ZhenX.MetallTransB,1993;24B:7899RansleyGE,NeufeldH.JInstMet,1948;74:59910CurtisRW,ChiottiP.JPhysChem,1963;67:1061z
[1] 厉英,丁玉石,崔绍刚,王常珍. 掺杂Sc的CaZrO3的制备及电学性能[J]. 金属学报, 2012, 48(5): 575-578.
[2] 厉英 丁玉石 胡井涛 王常珍. 用质子导体传感法研究钢在脱氢热处理中氢的行为[J]. 金属学报, 2011, 47(5): 553-558.
[3] 王东 刘春明 王常珍. 高温质子导体Ba3Ca1.18Nb1.82O9-δ的制备和表征[J]. 金属学报, 2009, 45(3): 345-350.