多弧离子镀Ti-N镀膜的扩散屏障作用
王家军;叶锐曾;孙榆芳
清华大学;北京科技大学;北京有色金属研究总院
ROLE OF MULTI-ARC PLATED Ti-N FILM AS A DIFFUSION BARRIER
WANG Jiajun(Tsinghua University; Beijing);YE Ruizeng(University of Science and Technology Beijing);SUN Yufang(General Research institute for Nonferrous Metals;Beijing)(Manuscript received 27 July;1993;in revised form 6 September 1993)
引用本文:

王家军;叶锐曾;孙榆芳. 多弧离子镀Ti-N镀膜的扩散屏障作用[J]. 金属学报, 1994, 30(14): 77-81.
, , . ROLE OF MULTI-ARC PLATED Ti-N FILM AS A DIFFUSION BARRIER[J]. Acta Metall Sin, 1994, 30(14): 77-81.

全文: PDF(374 KB)  
摘要: 设计了3种复合镀层系,研究了多弧离子镀Ti-N镀膜对Al,Ni,Co的扩散屏障作用及Ti-N镀膜在1000和1100℃长期时效时的热稳定化结果表明,在1000℃以下时效时,Ti-N镀膜稳定性良好,并可有效地阻止Al向基材扩散,可减缓、阻止Ni,Co在CoCrAlTaY涂层与基体间的互扩散行为;在1100℃时效时,Ti-N镀膜未分解,也不与基材及CoCrAlTaY涂层间发生互扩散,但组织形态由薄膜变为颗粒状,颗粒状Ti-N无法阻止Ni,Co在CoCrAlTaY涂层与基材间的互扩散.
关键词 : 包覆型涂层,  扩散屏障层,  互扩散效应,  Ti-N镀层    
Abstract:Several multi-layer coatings have been designed so as to assess the diffusion barriering ability against Al,Ni,Co,etc.as well as the high temperature stability of the multi-arc plated Ti-N film after being aged at 1000 and 1100℃ for a long time.The results show that,up to 1000℃,Ti-N film is of good stability;it can prevent effectively Al from diffusing towards matrix,and slow down the rate of diffusion of Ni,Co from CoCrAlTaY to matrix.Above 1100℃,the morphology of Ti-N film changes from thin foil to particles.Apparently the particle-shaped Ti-N can not prevent Ni,Co from the inter-diffusing between matrix and CoCrAlTaY coating.
Key words: overlaying coating    diffusion-barrier coating    inter diffusion effect    Ti-N coating
    
1GowardG.Trans ASM,1967;60:2282HsuLL.SurfCoatTechnol,1987;32:13RestallJE.In:Meethan G W ed.,TheDevelopmentofGasTurbineMaterials,London:AppliedScience.1981:2804王家军,叶锐曾,于文秀,孙庆标,马跃发,陈仁治.北京科技大学学报,1991;13:5795CoadJP,RickerbyD S,OberlanderN.MaterSciEng,1985;74:936Young SG,ZellarsGR.ThinSolidFilms,1978;53:2417王家军.北京科技大学硕士学位论文,1990J