金属学报  1994, Vol. 30 Issue (14): 72-76    
  论文 本期目录 | 过刊浏览 |
Sm_2(Fe_(1-x)Cr_x)_(17)N_(~2.7)永磁材料的结构与磁性能
周寿增;杨俊;张茂才;林毅;尹有祥;林国标
北京科技大学;北京矿冶研究总院
STRUCTURE AND MAGNETIC PROPERTIES OF Sm_2(Fe_(1-x)Cr_x)17N_(~2.7) MAGNETS
ZHOU Shouzeng;YANG Jun;ZHANG Maocai(University of Science and Technologl. Beijing);LIN Yi; YIN Youxiang;LIN Guobiao(Beijing General institute of Mining and Metallurgy)(Manuscript received 19 May;1993;in revised form 19 August;1993)
引用本文:

周寿增;杨俊;张茂才;林毅;尹有祥;林国标. Sm_2(Fe_(1-x)Cr_x)_(17)N_(~2.7)永磁材料的结构与磁性能[J]. 金属学报, 1994, 30(14): 72-76.
, , , , , . STRUCTURE AND MAGNETIC PROPERTIES OF Sm_2(Fe_(1-x)Cr_x)17N_(~2.7) MAGNETS[J]. Acta Metall Sin, 1994, 30(14): 72-76.

全文: PDF(360 KB)  
摘要: 研究了Cr部分取代Fe对Sm_2(Fe_(1-x)Cr_x)_17N_(~2.7)磁粉磁特性的影响.添加少量Cr(x=0-0.1),该化合物的结构不变化。随Cr含量的增加,它的Curie温度、各向异性场、饱和磁化强度、平均Fe原子磁矩和平均超精细场均有所降低.材料的单相性显著改善,矫顽力提高.Sm_2(Fe_(0.95)Cr_(0.05))_17N_(~2.7)磁粉的矫顽力_iH_c达到1592kA/m.
关键词 : SmFeN永磁,  氮化物磁体,  内禀磁特性    
Abstract:Effect of Cr in substitution for a part of Fe on structure and magnetic properties of Sm_2(Fe_(1-x)Cr_x)_(17)N_(~2.7) alloys powder has been investigated.The structure of the alloys remains the same with an addition of Cr,saying x=0-0.1.With the increase of Cr content,their Curie temperature,anisotropic field.saturation magnetization,average Fe atom moment and average hyperfine field decrease slightly.But their homogeneity may be obviously improved and coercivity increased even up to 1592 kA/m for Sm_2(Fe_0.95Cr_0.05)_17N_(~2.7) powder.
Key words: SmFeN magnet    nitride magnet    intrinsic magnetic property
    
1CoeyJMD,SunHong,HurelevDPF.J MagnMagnMater,1991;101:3102刘伟,王群,赵新国,赵彤,张志东,孙校开.金属学报,1993;29:B1263ZhouShouzeng,YangJun,ZhangMaocai,MaDeqing,LiFobiao,WangRun.In:Hi-permLaboratory,ResearchCentreforAdvancedMinoralandMaterialsProcessingeds.,Proc12thIntWorkshoponRareEarthMagnetsandTheirApplcations.TheUniversityofWersternAustralia,Nedland.Australia.1992:444DingJ,McCormichPG,StreetR,SmithPAL,In:Hi-permLaboratory,ResearchCentreforAdvancedMinoralandMaterialsProcessingeds.,Proc7thIntSymponMagneticAnisotropyandCoercivityinRE-TMAlloy,TheUniversityofWesternAustralia,Nedland,Australia,1992:4315KatterM,WeckerJ,KuhrtC,SchultzL.JMagnMagnMater,1992;117:4196YangJun,ZhouShouzeng,ZhangMaocai,LiFobiao,ZhaoJunhua,WangRun.MaterLett,1991;12:2427WalkerLR,WertheimGK,JaccarinaV.PhysRevLett,1961;6:988杨俊.北京科技大学博士学位论文,1992