Please wait a minute...
金属学报  1993, Vol. 29 Issue (8): 72-76    
  论文 本期目录 | 过刊浏览 |
等离子喷涂ZrO_2层经激光再熔后的组织变化
陈汉存;刘正义;庄育智
华南理工大学;华南理工大学;华南理工大学
STRUCTURAL CHANGE OF PLASMA SPRAYED ZrO_2 COATING AFTER LASER REMELTING
CHEN Hancun;LIU Zhengyi;ZHUANG Yuzhi South China University of Technology; Guangzhoudoctoral Department of Mechanical Engineering No.2; South China University of Technology;Guangzhou 510641
引用本文:

陈汉存;刘正义;庄育智. 等离子喷涂ZrO_2层经激光再熔后的组织变化[J]. 金属学报, 1993, 29(8): 72-76.
, , . STRUCTURAL CHANGE OF PLASMA SPRAYED ZrO_2 COATING AFTER LASER REMELTING[J]. Acta Metall Sin, 1993, 29(8): 72-76.

全文: PDF(1183 KB)  
摘要: 本文研究了等离子喷涂ZrO_2陶瓷层的激光再熔化处理经激光再熔化处理的ZrO_2涂层致密、无孔隙,但熔化层有裂纹在ZrO_2中添加适量的SiO_2,降低了熔化层在冷却时的热应力,有效抑制裂纹的产生经激光再熔化处理后的陶瓷展和粘结层之间的结合为冶金结合;粘结尾和基材的冶金结合层厚度明显增加;随着激光功率的增加,陶瓷层、粘结层以及一定厚度的基材发生熔化,陶瓷层和粘结层之间产生Zr_6Fe_3O反应相
关键词 : 等离子喷涂,  ZrO_2涂层,  激光处理,  SiO_2    
Abstract:An improvement on the properties of plasma sprayed ZrO_2 ceramic coatingby laser remelting treatment has been observed by TEM, SEM, EPMA and X-ray diffractionanalysis. After laser remelting, the ZrO_2 coating changes its structure into more dense andnonporous, and more stable to thermal failure and cracking if a suitable SiO_2 doped. Thebonding of laser remelted ZrO2 ceramic coating together with adhesion layer is found to be ofmetallurgical nature. The thickness of adhesion layer and metallurgical bonding interface maybe evidently increased. With the increase of the laser output, the ceramic coating, adhesionlayer and a certain depth of substrate surface are able to be fused. A liquid Zr6Fe3o phase maybe formed between ceramic coating and adhesion layer.
Key words: plasma spraying    ZrO_2 coating    laser remelting    SiO_2
收稿日期: 1993-08-18     
1 陈汉存,刘正义,庄育智,关侃.材料科学进展,1992;6:146
2 Chen Hancun, Liu Zhengyi, Zhuang Yuzhi, Xu Linkang. Chin J Mech Eng, 1992; 5(3) : 183
3 Sivakumar R, Mordike B L. Surf Eng. 1988; 4: 127
4 Galasso F S, Veltri R. Ceram Bull, 1983; 62: 253
5 Zaplatynsky I. Thin Solid Films, 1982: 95: 275
6 Adamski A, McPherson R. In: Welding Institute of Canada ed., Advances in Thermal Spraying, Proc. 11th Int. Thermal Spraying Conf, Montreal, Canada, Sept. 8--12, 1986: 555, Canade: Pergamon Press
7 Iwamoto N, Umesaki N, Endo S. In: Welding Institute of Canada ed., Advances in Thermal Spraying, Proc. 11th Int. Thermal Spraying Conf, Montreal, Canada, Sept. 8--12, 1986: 563, Canade: Pergamon Press
8 Havrda M, Volenik K, Wagner J, Mraz P. In: Welding Institute of Canada ed., Advances in Thermal Spraying, Proc. 11th Int. Thermal Spraying Conf., Montreal, Canada, Sept.8--12, 1986: 569, Canade: Pergamon Press
[1] 董昕远, 雒晓涛, 李成新, 李长久. B清除大气等离子喷涂CuNi熔滴氧化物效应[J]. 金属学报, 2022, 58(2): 206-214.
[2] 李晓倩, 王富国, 梁爱民. 喷涂工艺对Ta2O5原位复合钽基纳米晶涂层微观结构及摩擦磨损性能的影响[J]. 金属学报, 2021, 57(2): 237-246.
[3] 宫文彪,李任伟,李于朋,孙大千,王文权. CeO2/ZrO2-Y2O3纳米结构热障涂层的高温稳定性及耐腐蚀性能[J]. 金属学报, 2013, 49(5): 593-598.
[4] 付翀,王俊勃,杨敏鸽,侯锦丽,丁秉钧. 等离子喷涂Ag/(Sn0.8La0.2)O2涂层的组织及电性能[J]. 金属学报, 2013, 49(3): 325-329.
[5] 项建英 陈树海 黄继华 赵兴科 张华. 等离子喷涂La2(Zr0.7Ce0.3)2O7热障涂层的抗热震性能[J]. 金属学报, 2012, 48(8): 965-970.
[6] 刘静 盛洪飞 张保山 彭良明. 含等离子喷涂ZrO2热障涂层的Ti3XC2(X=Al, Si)性能研究[J]. 金属学报, 2011, 47(9): 1141-1146.
[7] 徐娜 张甲 侯万良 全明秀 李荣德 常新春. 热处理对高温固体自润滑涂层组织结构及结合强度的影响[J]. 金属学报, 2009, 45(8): 943-948.
[8] 潘冶; 王春明; 郑仲瑜; 佟晓辉 . 等离子喷涂纳米SiCf/FeS复合涂层的摩擦学性能[J]. 金属学报, 2008, 44(4): 463-466 .
[9] 王存山; 高亚丽; 姚曼 . 镁合金AZ91HP表面激光重熔Al2O3涂层的组织及性能[J]. 金属学报, 2007, 43(5): 493-497 .
[10] 吕宇鹏; 李士同; 梁栋科; 朱瑞富; 李木森; 雷廷权 . 等离子体熔融钛与羟基磷灰石混合粉颗粒的形态和相组成[J]. 金属学报, 2002, 38(12): 1292-1294 .
[11] 王凤平;王佩璇;方正知;崔明启;姜晓明;马宏骥. Mo/SiO_2软X射线多层膜反射镜的界面分析[J]. 金属学报, 1997, 33(7): 737-741.
[12] 张晓兵;蒋国昌;徐匡迪. 高阶亚正规溶液模型及其在MnO-SiO_2-Al_2O_3-CaO炉渣中组元活度的计算[J]. 金属学报, 1997, 33(10): 1085-1093.
[13] 黄宗泽;肖兴国;肖泽强. CaO-SiO_2-Al_2O_3-FeO熔渣起泡行为的研究[J]. 金属学报, 1995, 31(19): 289-294.
[14] 张培新;张奇志;吴黎明;隋智通. 用神经网络─遗传算法优化MgO-B_2O_3─SiO_2渣系组成[J]. 金属学报, 1995, 31(18): 284-288.
[15] 杨学民;郭占成;于宪溥;艾菁;王大光. CO还原CaO-SiO_2-Al_2O_3-Fe_tO渣系研究[J]. 金属学报, 1994, 30(23): 491-498.