| TiB_2-xAl复合体系的SHS合成过程研究 |
| 傅正义;袁润章;MunirZA |
| 副教授;武汉(430070);武汉工业大学材料复合新技术国家实验室;武汉工业大学;UniversityofCalifornia;Davis |
|
| SELF-PROPAGATION HIGH-TEMPERATURE SYNTHESIS OF TiB_2-χAl COMPOSITE SYSTEM |
| FU Zhengyi;YUAN Runzhang;MUNIR Zuhair A Wuhan University of Technology University of California; Davis; USA Wuhan University of Technology; Wuhan 430070 |
引用本文:
傅正义;袁润章;MunirZA. TiB_2-xAl复合体系的SHS合成过程研究[J]. 金属学报, 1993, 29(7): 92-96.
,
,
.
SELF-PROPAGATION HIGH-TEMPERATURE SYNTHESIS OF TiB_2-χAl COMPOSITE SYSTEM[J]. Acta Metall Sin, 1993, 29(7): 92-96.
1 傅正义、袁润章:武汉工业大学学报,1992;13(2) :26 2 Yuan R Z, Fu Z Y, Munir Z A, J Mater Synthesis and Processing, 1993; 3. 153 3 Fu Z Y, Yuan R Z, Yang Z L, Proceedings of the 1st Inter. Sym. on FGM, Japan, 1990; 175. 4 Munir Z A, Ceram Bull, 1988: 67: 342. 5 Fu Z Y, Yuan R Z, Wang W M, Solid State Phenomena, 1992; 25&26: 209. 6 Fu Z Y, Yuan R Z, Munir Z A, Inter J SHS, 1992; 1: 119.Y |
|