N-羟基邻苯二甲酰亚胺对氟碳铈矿的浮选性能及其作用机理
任俊
冶金工业部包头稀土研究院;工程师;包头014010
FLOTATION BEHAVIOUR AND MECHANISM OF BASTNAESITE WITH N-HYDROXYLE PHTHALICIMIDE
REN Jun Baotou Research Institute of Rare Earth Metals; Ministry of Metallurgical Industry engineer;Baotou Research Institute of Rare Earth Metals Baotou 014010
引用本文:

任俊. N-羟基邻苯二甲酰亚胺对氟碳铈矿的浮选性能及其作用机理[J]. 金属学报, 1993, 29(6): 49-53.
. FLOTATION BEHAVIOUR AND MECHANISM OF BASTNAESITE WITH N-HYDROXYLE PHTHALICIMIDE[J]. Acta Metall Sin, 1993, 29(6): 49-53.

全文: PDF(370 KB)  
摘要: 通过?-电位,红外光谱及量子化学计算结果研究了N-羟基邻苯二甲酰亚胺对氟碳铈矿的浮选性能结果表明,前者对氟碳铈矿具有良好的浮选选择性,它是以三个氧原子为键合原子与氟碳铈矿表面的RE(Ⅲ)螯合形成O=C-N-O-RE(Ⅲ)-O双五元环螯合物而化学吸附在其表面
关键词 : N-羟基邻苯二甲酰亚胺,  捕收剂,  氟碳铈矿,  浮选,  作用机理    
Abstract:The flotation behaviour and mechanism of bastnaesite with N-hydroxylphthalicimide were investigated by ζ-potential measurement, infrared spectrum and quantumchemistry calculation. The results show that 3 oxygen atoms from N-hydroxyl phthalicimidechelate the rare earh ions on the surface of bastnaesite to form double five-chainO=C-N-O-RE (Ⅲ)-O chelate which is chemically adsorbed on the surface of bastnaesite,thus making N-hydroxyl phthalicimide an effective collector for bastnaesite.
Key words: N-hydroxyl phthalicimide    flotation    bastnaesite    collector
收稿日期: 1993-06-18     
1 Плакин И Н,Мелкнх В И.国外金属矿选矿,1964;(5) :21
2 Двормиченко Д И.国外金属矿选矿,1974;(7--8) :29
3 向井滋.浮选,1984;(31) :209
4 许时.矿石可选性研究.北京:冶金工业出版社,1981:252
5 古映莹,朱玉霜.稀有金属,1988;7(2) :81\
[1] 孙水裕;王淀佐;李柏淡. 无捕收剂浮选时硫化矿物表面的疏水-亲水平衡关系[J]. 金属学报, 1993, 29(9): 53-59.
[2] 刘亚川;龚焕高;张克仁;田喜林. 油酸在石英与长石表面的吸附[J]. 金属学报, 1993, 29(11): 49-53.