    					| Nd—Fe—B和Pr—Fe—B相图三维拓扑分析 |  
						| 刘国权;徐平国 |  
					| 北京科技大学材料科学与工程系金相教研室;教授;北京100083;北京科技大学 |  
						|  |  
    					| THREE-DIMENSIONAL TOPOLOGICAL ANALYSIS OF Nd-Fe-B AND Pr-Fe-B PHASE DIAGRAMS |  
						| LIU Guoquan;XU Pingguo University of Science and Technology Beijing professor;University of Science and Technology Beijing; Beijing 100083 |  
								刘国权;徐平国. Nd—Fe—B和Pr—Fe—B相图三维拓扑分析[J]. 金属学报, 1993, 29(3): 57-61.	
																												,
																												 . 
				THREE-DIMENSIONAL TOPOLOGICAL ANALYSIS OF Nd-Fe-B AND Pr-Fe-B PHASE DIAGRAMS[J]. Acta Metall Sin, 1993, 29(3): 57-61.
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| 1 Hillert M. Int: Metals Rev, 1985: 30 (2) : 45 2 Rhines F N. Phase Diagrams in Metallurgy. New York: McGraw-Hill, 1956; 204
 3 Matsuura Y, Hirosawa S, Yamamoto H, Fujimura S, Sagawa M, Osamura K. Jpn J Appl Phys. 1985; 24: L635
 4 张宁,罗阳,金属学报.1989;25:B104
 5 张宁,罗阳,金属学报.1989;25:B109
 6 车广灿,梁敬魁,王选章,中国科学.1985;A(10) :909
 7 Schneider G, Henig E-T, Petzow G, Stadelmaier H H. Z Metallkde, 1986; 77: 755
 8 Henig E-T. Schneider G. Stadelmaier H H. Z Metallkde, 1987: 78 (11) : 818
 9 Zhang W, Liu G, Han K. In: Massalski et al. eds., Binary Alloy Phase Diagrams. 2nd ed. ASM International, 1990; 1732
 1O 徐平国,北京科技大学硕士学位论文,1991;79
 11 Hao S. Xu W. J Chin Rare Earth Soc. 1990; 8 (3) : 200
 12 田静华,黄毅英,梁敬魁,中国科学.1987;A(2) :159S
 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |