Please wait a minute...
金属学报  1993, Vol. 29 Issue (10): 10-16    
  论文 本期目录 | 过刊浏览 |
Fe—Cr—Mn(Ni)合金抗辐照损伤特性研究
胡本芙;高桥平七郎
北京科技大学;日本北海道大学
BEHAVIOURS OF RESISTANCE TO IRRADIATED DAMAGE IN Fe-Cr-Mn(Ni) ALLOYS
HU Benfu;TAKAHASHI;Heishichiro University of Science and Technology Beijing Hokkaide University; Japan
引用本文:

胡本芙;高桥平七郎. Fe—Cr—Mn(Ni)合金抗辐照损伤特性研究[J]. 金属学报, 1993, 29(10): 10-16.
, . BEHAVIOURS OF RESISTANCE TO IRRADIATED DAMAGE IN Fe-Cr-Mn(Ni) ALLOYS[J]. Acta Metall Sin, 1993, 29(10): 10-16.

全文: PDF(1983 KB)  
摘要: 电子束辐照结果证明、Fe-Cr—Mn合金辐照损伤行为不同于Fe—Cr—Ni合金、因为溶质原子与点缺陷有相互作用,特别是Mn原子与空位相互作用比Ni原子来得强烈、致使Fe—Cr—Mn合金中空位迁移激活能比Fe—Cr—Ni合金高Ni,Mn在合金中扩散行为不同,是造成两种合金辐照损伤行为不同的原因
关键词 : 电子辐照,  空位迁移激活能,  Fe—Cr—Mn(Ni)合金    
Abstract:The damage behaviour of Fe-Cr-Mn alloys during electron irradiation isshown to be different from that in Fe-Cr-Ni alloy. The difference appears to be a conse-quence of the different diffusion behaviour of Ni and Mn due to interaction between soluteatoms and point defects. Especially the interaction between Mn atoms and vacancies inFe-Cr-Mn is strong so that the migration energy becomes greater than that in Fe-Cr-Ni al-
Key words: electron irradiation    migration energy    Fe-Cr-Mn (Ni) alloy
收稿日期: 1993-10-18     
1 Brager H R, Garner F A, Gelles D S, Hamilton M L. J Nucl Mater, 1985; 133--134: 907
2 Takahashi H, Takeyama T, Tanikawa K, Miura R. J Nucl Mater. 1985; 133--134: 566
3 Takahashi H, Ohnuki S, Kinoshita H, Nakahigashis. J Nucl Mater, 1991; 179--181: 629
4 桐谷道雄.金属学会会志,1967;8:553
5 Watanabe H, Aoki A, Murakami H, Yoshida N. J Jpn Inst Met, 1988; 152: 536
6 Kiritani M, Yoshida N, Takata H, Machara Y. J phy Soc Jpn, 1975; 138: 1677
7 Kiritani M, Takata H, Moriyama K, Eiich Jujita F. Phylos Mag 1979: A40: 779
8 Rehn L E, Okamoto P R, Potter D L, Wiedersich H. J Nucl Mater, 1978; 74: 242
9 Deschepper L, Cornells J, Knuyt G, Nihoul J, Stals L. Phys status solidi, 1980; (a) 61: 3
10 Tabata T, Fujita H, Igaki K, Isshiki M, Scr Met, 1981; 14: 1317
11 胡本芙,高桥平六郎,竹山太郎,金属学报,1990;26:1V
[1] 胡本芙;吴承健. 新型抗辐照氧化物弥散强化(ODS)型铁素体不锈钢辐照损伤特性研究[J]. 金属学报, 1995, 31(11): 525-530.
[2] 万发荣;肖纪美;袁逸. 利用电子束辐照方法测定空位迁移能[J]. 金属学报, 1990, 26(2): 74-78.
[3] 胡本芙;高桥平七郎;竹山太郎. 电子辐照Fe-Cr-Ni奥氏体合金的空洞体胀与诱起晶界偏析的研究[J]. 金属学报, 1988, 24(3): 180-186.