| 辉光放电灯中二元合金溅射率与化学组成的关系 |
| 任建世;张功杼;王桢枢;刘根;刘圣麟 |
| 中国科学院金属研究所;中国科学院金属研究所;高级工程师;沈阳(110015)中国科学院金属研究所;上海工业大学;上海工业大学;上海工业大学 |
|
| CORRELATION BETWEEN CONSTITUENT AND SPUTTERING RATE OF BINARY ALLOYS IN GLOW DISCHARGE LAMP |
| REN Jianshi;ZHANG Gongshu;WANG Zhenshu;LIU Gen;LIU Shenglin Institute of Metal Research; Academia Sinica; Shenyang; Shanghai University of Technology Correspondent senior engineer; Institute of Metal Research; Academia Sinica; Shenyang 110015 |
引用本文:
任建世;张功杼;王桢枢;刘根;刘圣麟. 辉光放电灯中二元合金溅射率与化学组成的关系[J]. 金属学报, 1992, 28(5): 85-89.
,
,
,
,
.
CORRELATION BETWEEN CONSTITUENT AND SPUTTERING RATE OF BINARY ALLOYS IN GLOW DISCHARGE LAMP[J]. Acta Metall Sin, 1992, 28(5): 85-89.
1 Boumans P W J M. Anal Chem, 1972; 44: 1219 2 任建世,赵惠林,张功抒.中国专利,88217038. 4,1988 3 Greene JE, Natarajan B R, Sequeda-Osorio F. J Appl Phys, 1978; 49: 417 4 任建世,张功杼.分析化学,1983;11:586 5 Pons-Corbeau J. Surf Interface Anal, 1985; 7: 169 6 Pons-Corbeau J. Surf Interface Anal, 1986; 9: 21 7 刘圣麟,张功杼,任建世,王桢枢.中国商检,1991;(116) : |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|