| 电动势法测定Na_2SnO_3的生成自由能 |
| 郑敏辉;陈一松 |
| 北京科技大学;副研究员;北京(100083)北京科技大学理化系冶金物化教研室;北京科技大学 |
|
| 0412-1961 |
| FREE ENERGY OF FORMATION OF Na_2SnO_3 BY EMF MEASUREMENT USING β-ALUMINA SOLID ELECTROLYTE CELL |
引用本文:
郑敏辉;陈一松. 电动势法测定Na_2SnO_3的生成自由能[J]. 金属学报, 1992, 28(2): 91-93.
,
.
0412-1961[J]. Acta Metall Sin, 1992, 28(2): 91-93.
1 矢彬.非铁金属制鍊.日本金属学会,1982:137 2 Zheng Minhui, Zhong kai. In: Chowda R I, Liu Q G, Chen L Q eds., Recent Advances in Fast Ion Conducting Materials and Devices, Proc of the Conf, held at Beijing, October 28-November 1, 1990: 481 3 Sjoden O, Seetharaman S, Staffansson L-I. Metall Trans, 1986; 17B: 179 4 Venugopal V, Iyer V S, Sundaresh V, Singh Z, Prasad R, Sood D D. J Chem Thermody, 1987; 19: 19 |
|