| 1Cr18Ni9不锈钢精细结构分析 |
| 滕凤恩;王煜明;徐跃 |
| 吉林大学;吉林大学;吉林大学 |
|
| FINE STRUCTURE ANALYSIS OF DEFORMED AUSTENITE STAINLESS STEEL 1Cr18Ni9 |
| TENG Feng'en;WANG Yuming;XU Yue Jilin University; Chang chun |
引用本文:
滕凤恩;王煜明;徐跃. 1Cr18Ni9不锈钢精细结构分析[J]. 金属学报, 1992, 28(1): 45-47.
,
,
.
FINE STRUCTURE ANALYSIS OF DEFORMED AUSTENITE STAINLESS STEEL 1Cr18Ni9[J]. Acta Metall Sin, 1992, 28(1): 45-47.
1 桑野三郎.材料,1977;26(287) :735--741 2 Nair PK, Vasudevan R. J Appl Crystallogr, 1977; 10: 401--404 3 滕凤恩,王煜明.理化检验(物理分册),1989;(2) :40--49 4 滕凤恩,崔相旭.物理学报,1989;38:1845--1848 5 Tung Feng-en (Teng Feng'en), Wang Yuming. J Mater Sci, 1986; 21: 3223--3226* |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|